首页> 外文期刊>Carbohydrate Polymers: Scientific and Technological Aspects of Industrially Important Polysaccharides >Polycaprolactone and polycaprolactone/chitosan nanofibres functionalised with the pH-sensitive dye Nitrazine Yellow
【24h】

Polycaprolactone and polycaprolactone/chitosan nanofibres functionalised with the pH-sensitive dye Nitrazine Yellow

机译:pH敏感染料硝嗪黄功能化的聚己内酯和聚己内酯/壳聚糖纳米纤维

获取原文
获取原文并翻译 | 示例

摘要

Nanofibres functionalised with pH-sensitive dyes could greatly contribute to the development of stimuli-responsive materials. However, the application of biocompatible polymers is vital to allow for their use in (bio)medical applications. Therefore, this paper focuses on the development and characterisation of pH-sensitive polycaprolactone (PCL) nanofibrous structures and PCL/chitosan nanofibrous blends with 20% chitosan. Electrospinning with added Nitrazine Yellow molecules proved to be an excellent method resulting in pH-responsive non-wovens. Unlike the slow and broad response of PCL nanofibres (time lagof more than 3 h), the use of blends with chitosan led to an increased sensitivity and significantly reduced response time (time lag of 5 min). These important effects are attributed to the increased hydrophilic nature of the nanofibres containing chitosan. Computational calculations indicated stronger interactions, mainly based on electrostatic interactions, of the dye with chitosan (ΔG of-132.3 kJ/mol) compared to the long-range interactions with PCL(ΔG of-35.6 kJ/mol), thus underpinning our experimental observations. In conclusion, because of the unique characteristics of chitosan, the use of PCL/chitosan blends in pH-sensitive biocompatible nanofibrous sensors is crucial.
机译:用pH敏感染料功能化的纳米纤维可以极大地促进刺激反应性材料的开发。但是,生物相容性聚合物的应用对于使其用于(生物)医学应用至关重要。因此,本文着重于对pH敏感的聚己内酯(PCL)纳米纤维结构以及PCL /壳聚糖纳米纤维与20%壳聚糖的共混物的开发和表征。添加了硝基嗪黄分子的静电纺丝被证明是一种出色的方法,可产生对pH敏感的无纺布。与PCL纳米纤维的响应缓慢而宽泛(滞后时间超过3小时)不同,与壳聚糖共混的使用可提高灵敏度并显着减少响应时间(滞后时间为5分钟)。这些重要作用归因于含有壳聚糖的纳米纤维的亲水性增加。计算结果表明,与壳聚糖的染料相互作用(ΔG为-35.6 kJ / mol)与染料与壳聚糖的相互作用更强,主要是基于静电相互作用(ΔG为-132.3 kJ / mol),从而支持了我们的实验观察。总之,由于壳聚糖的独特特性,在对pH敏感的生物相容性纳米纤维传感器中使用PCL /壳聚糖混合物至关重要。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号