Recovery of molybdenum from roasted copper slags

机译:从烤铜渣中回收钼

获取原文
获取原文并翻译 | 示例
       

摘要

Recycling copper slag to recover metals has been focused on copper, which is contained in the range of 0.77 to 1.32%; however some slags also contains molybdenum in amount up to 0.4% transforming the copper smelting slags into a potential raw material for the development of new processes to obtain new products. In this regard, copper slags were treated using roasting-leaching process in order to recover the molybdenum content in the slag. Oxidative roasting is used to convert the iron oxide into insoluble hematite, and copper and molybdenum into the soluble form in acidic solution. Since molybdenum is associated to iron oxide spinel type phase, its recovery was influenced by the magnetite content in the slag during the leaching process. Sulphuric acid was used for leaching the slag, and molybdenum shows recovery higher than 80%. Thus, the obtained results show the feasibility for recovering molybdenum using two-step processes, oxidative roasting followed by an acidic leaching.
机译:回收铜渣以回收金属的重点是铜,其含量范围为0.77%至1.32%;然而,某些炉渣还含有高达0.4%的钼,从而将铜冶炼炉渣转化为潜在的原材料,可用于开发新工艺以获得新产品。在这方面,为了回收炉渣中的钼,使用了焙烧-浸出法处理了铜炉渣。氧化焙烧用于在酸性溶液中将氧化铁转化为不溶性赤铁矿,并将铜和钼转化为可溶形式。由于钼与氧化铁尖晶石型相相关,因此在浸出过程中,其回收率受炉渣中磁铁矿含量的影响。硫酸用于浸出炉渣,钼的回收率高于80%。因此,获得的结果表明使用两步法,氧化焙烧,然后进行酸性浸提来回收钼的可行性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号