Long-term clinical results of galvano-ceramic and glass-ceramic individual crowns.

机译:电陶瓷和玻璃陶瓷单个牙冠的长期临床结果。

获取原文
获取原文并翻译 | 示例

摘要

STATEMENT OF PROBLEM: Alternatives to metal-ceramic restorations should possess clinical durability before being recommended to the dentist. Longitudinal clinical studies are required for evaluation so innovative types of restorations can meet the expectations of dentists and patients. PURPOSE: This study compared the performance of galvano-ceramic restorations (Auvo Galvano Crown [ACG]) and glass-ceramic individual crowns (Dicor) based on longitudinal clinical trials. MATERIAL AND METHODS: A total of 769 galvano-ceramic single crowns (AGC) in 322 patients and 173 glass-ceramic individual crowns (Dicor) in 88 patients were reviewed for 8 years and a maximum of 11 years, respectively, after cementation. Risk of fracture was determined with use of a survival analysis (Kaplan and Meier). RESULTS: Partial ceramic cracking was observed at the time of the last recording of data in 11 galvano-ceramic crowns, 8 of the units remained in place. Two crowns became dislodged and 1 tooth exhibited a fractured root, despite an intact crown. One restoration was removed because of hypersensitivity and 1 with partial ceramic fracture. Forty-two of the glass-ceramic crowns were completely fractured. After a comparable 7 years under risk, 96.5% (+/-3.4; 95% confidence interval) of the galvano-ceramic premolar and molar crowns and 92% (+/- 8.5) of crowns placed on incisors and canines crowns were intact. The corresponding data for the glass-ceramic restorations were only 70% (+/- 10.6) in posterior and 82.7% (+/- 8. 1) in anterior quadrants. CONCLUSION: Long-term results of electroformed individual crown restorations were superior to glass-ceramic restorations.
机译:问题陈述:在推荐给牙医之前,金属陶瓷修复体的替代品应具有临床耐久性。评估需要进行纵向临床研究,以便创新的修复体类型能够满足牙医和患者的期望。目的:本研究根据纵向临床试验比较了电瓷修复体(Auvo Galvano Crown [ACG])和玻璃陶瓷单个牙冠(Dicor)的性能。材料与方法:胶结后,分别对322例患者中的769个电瓷单冠(AGC)和88例患者中的173个玻璃陶瓷单冠(Dicor)进行了8年和最长11年的回顾。使用生存分析(Kaplan和Meier)确定骨折风险。结果:在最后一次记录11个电瓷冠中的数据时,观察到部分陶瓷开裂,其中8个仍保留在原位。尽管牙冠完好无损,但有两个牙冠脱落,并且1个牙齿的根部骨折。由于超敏反应,移除了一个修复体,其中1个修复体部分陶瓷破裂。 42个玻璃陶瓷冠完全断裂。在经历了可比的7年危险之后,完整的95.6%(+/- 3.4; 95%置信区间)的电陶瓷前磨牙和磨牙冠以及92%(+/- 8.5)的门牙和犬齿冠完好无损。玻璃陶瓷修复体的相应数据在后象限仅为70%(+/- 10.6),在前象限仅为82.7%(+/- 8. 1)。结论:电铸单个牙冠修复体的长期效果优于玻璃陶瓷修复体。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号