Synergistic effect of oil palm ash filled natural rubber compound at low filler loading

机译:低填充量下油棕灰填充天然橡胶胶料的协同作用

获取原文
获取原文并翻译 | 示例
           

摘要

This work studied the possibility of utilizing oil palm ash (OPA) as filler to reinforce natural rubber (NR) compounds. The OPA loading used in this study ranged from 0 to 9 phr. The properties of low filler loading OPA filled natural rubber were investigated in terms of curing characteristics, tensile properties, rubber-filler interaction and morphology of tensile fractured surface. From the results, it was observed that the scorch and cure times decreased with the addition of OPA whereas maximum torque, tensile modulus (M_(100) and M_(300)) and hardness increased. With the addition of OPA, it was worthwhile to note that the tensile strength and elongation at break improved 16% and 7.4%, respectively, up to an optimum level of 1 phr. Beyond this point, there was a detrimental effect on the strength and flexibility due to agglomeration of hydrophilic OPA. The measurement of rubber-filler interaction by FT-IR and morphological studies of tensile fracture surface of oil palm ash filled natural rubber vulcanizates supported the result obtained from tensile properties.
机译:这项工作研究了利用油棕灰(OPA)作为填料来增强天然橡胶(NR)化合物的可能性。本研究中使用的OPA负载范围为0至9 phr。从硫化特性,拉伸性能,橡胶与填料的相互作用以及拉伸断裂表面的形态等方面研究了低填料含量的OPA填充天然橡胶的性能。从结果可以看出,随着加入OPA,焦烧和固化时间减少,而最大扭矩,拉伸模量(M_(100)和M_(300))和硬度增加。通过添加OPA,值得注意的是,拉伸强度和断裂伸长率分别提高了16%和7.4%,最高达1 phr。超过这一点,由于亲水性OPA的团聚,对强度和柔韧性产生不利影响。用傅立叶变换红外光谱(FT-IR)进行的橡胶-填料相互作用测量以及油棕灰填充的天然橡胶硫化胶的拉伸断裂表面形态研究证明了从拉伸性能获得的结果。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号