EIS study on failure process of two polyurethane composite coatings

机译:两种聚氨酯复合涂料失效过程的EIS研究

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

The performance of acrylic polyurethane composite coating and aliphatic urethane composite coating in 3.5% NaCl solution under ultra-violet radiation was studied with methods of EIS, SEM and FTIR. For aliphatic polyurethane coating, the coating resistance decreased and the coating capacitance and porosity increased more quickly than acrylic polyurethane coating. The acrylic polyurethane composite coatings showed better performance than aliphatic polyurethane composite coatings. IR spectra showed that under UV irradiation conditions, the failure mechanism of the two polyurethane coatings was the transformation of sec-amide to primary amides. The fractured bonds in acrylic polyurethane were mainly C-O bonds, while in aliphatic polyurethane they were mainly C-N bonds. The lower protection property of aliphatic polyurethane coating may be mainly attributed to the C-N bonds which are more liable to be broken.
机译:采用EIS,SEM和FTIR方法研究了丙烯酸聚氨酯复合涂料和脂肪族聚氨酯复合涂料在3.5%NaCl溶液中的紫外辐射性能。对于脂族聚氨酯涂料,与丙烯酸聚氨酯涂料相比,涂层电阻降低,涂层电容和孔隙率增加更快。丙烯酸聚氨酯复合涂料表现出比脂肪族聚氨酯复合涂料更好的性能。红外光谱表明,在紫外光照射条件下,两种聚氨酯涂料的破坏机理为仲酰胺向伯酰胺的转化。丙烯酸聚氨酯中的断裂键主要是C-O键,而脂肪族聚氨酯中的断裂键主要是C-N键。脂肪族聚氨酯涂料的较低的保护性能可能主要归因于更易于断裂的C-N键。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号