Influence of stem type on material loss at the metal-on-metal pinnacle taper junction

机译:阀杆类型对金属对金属顶峰锥形结处材料损失的影响

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

The clinical importance of material loss at the head-stem junction is unknown. Comparison of retrievals with different stem types can provide the opportunity to understand the importance of the taper junction. This was a case-control study involving 20 retrieved 36 mm metal-on-metal Pinnacle (DePuy) hips that were paired with either a Corail (n = 10) or S-ROM (n = 10) stem. The median head taper material loss rate for the Corail group was 0.238 (0.0002-2.178) mm(3)/year and was significantly greater than the S-ROM group (p = 0.042), which had a median material loss rate of 0.132 (0.015-0.518) mm(3)/year. The only significant difference between the groups was the stem taper roughness and length: this was rougher and shorter for the Corails. Long and smooth stem taper designs are preferred when used in conjunction with metal heads.
机译:头干交界处物质损失的临床重要性尚不清楚。比较具有不同茎类型的取回可以提供机会来了解锥形连接的重要性。这是一个病例对照研究,涉及20根取回的36毫米金属对金属尖顶(DePuy)髋部,与Corail(n = 10)或S-ROM(n = 10)茎配对。 Corail组的平均头部锥度材料损失率为0.238(0.0002-2.178)mm(3)/年,并且显着大于S-ROM组(p = 0.042),后者的平均材料损失率为0.132( 0.015-0.518)mm(3)/年。两组之间唯一的显着差异是杆锥度的粗糙度和长度:这对于Corails而言更粗糙,更短。与金属头结合使用时,长而光滑的杆锥度设计是首选。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号