In this work, rubber powders were obtained by spraydrying of styrene-butadiene latex modified with a colloidal oxide, methyl methacrylate and sodium 4-styrene sulfonate. After the modification step, the particle size of latex dispersions was determined by photon correlation spectroscopy and showed an average diameter of about 100 nm. The latex dispersions were spray dried to obtain a particulate rubber. After the drying process, the morphology of the rubber powder particles was evaluated by scanning electronic microscopy. The micrographs revealed a coalesced system for unmodified styrene-butadiene latex and particulate systems for modified lattices containing colloidal oxide, both dried in the same conditions. The particle size of rubber powders analyzed by scanning electronic microscopy ranged from approximately 1 μm to 10μm. Differential scanning calorimeter analysis indicated that the glass transition temperatures did not change significantly, and thermogravimetric analysis showed thermal stability until approximately 200 °C
机译:在这项工作中,通过对用胶体氧化物,甲基丙烯酸甲酯和4-苯乙烯磺酸钠改性的苯乙烯-丁二烯胶乳进行喷雾干燥,获得了橡胶粉。在改性步骤之后,通过光子相关光谱法确定胶乳分散体的粒径,并显示出约100nm的平均直径。将胶乳分散体喷雾干燥以获得粒状橡胶。在干燥过程之后,通过扫描电子显微镜评价橡胶粉末颗粒的形态。显微照片揭示了未改性的苯乙烯-丁二烯胶乳的聚结体系和含有胶体氧化物的改性晶格的颗粒体系,二者均在相同条件下干燥。通过扫描电子显微镜分析的橡胶粉末的粒度为约1μm至10μm。差示扫描量热仪分析表明玻璃化转变温度没有显着变化,热重分析显示直到约200°C的热稳定性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号