Fibre orientation of fibre-reinforced PBT composites in injection moulding

机译:纤维增强PBT复合材料在注塑中的纤维取向

获取原文
获取原文并翻译 | 示例
           

摘要

The present study investigates the fibre orientation and distribution of 15wt-% short fibre-reinforced polybutylene terephthalate using both experimentation and computer-aided analysis. Filling time, melt temperature, mould temperature and packing pressure are chosen to be the controllable parameters that govern the injection-moulding process. The influence of injection-moulding process parameters on the frozen-intermediate-core morphology is observed using scanning electron microscopy. The variations of frozen layer thickness are strongly affected by the injection-moulding parameters. The minimum is at a filling time of 3 s, a melt temperature of 240℃, a mould temperature of 90℃, and a packing pressure of 100% of the constant 42 MPa injection pressure for the mould with dimension 45 mm × 45 mm × 4.0 mm. The experimental results are used to validate the accuracy of the computer simulation in fibre orientation and distribution. Simulated and experimental results closely correspond to each other.
机译:本研究使用实验和计算机辅助分析方法研究了15wt%的短纤维增强聚对苯二甲酸丁二醇酯的纤维取向和分布。选择填充时间,熔体温度,模具温度和填充压力作为控制注塑过程的可控制参数。使用扫描电子显微镜观察了注塑工艺参数对冷冻中间核形态的影响。冷冻层厚度的变化受到注塑参数的强烈影响。最小值为3 s的填充时间,熔融温度为240℃,模具温度为90℃,填充压力为尺寸为45 mm×45 mm×的模具的恒定42 MPa恒定注射压力的填充压力的100%。 4.0毫米实验结果用于验证计算机模拟在纤维取向和分布方面的准确性。模拟结果和实验结果彼此接近。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号