The main focus of this study is to examine and evaluate the effect of Fe, Ni and Cr on the corrosion?behaviour of hypereutectic Al-Si automotive alloy in 3.5% NaCl solution. Experimental information are attained?using conventional gravimetric measurements under different solution temperature and velocity and?complemented by resistivity, optical micrograph, scanning electron microscopy (SEM) and X-ray analyzer (EDX)?investigations. All the alloys show the negative corrosion rate due to formation of a very thin film of aluminum?oxide and hydroxid on the surface. Intermetallic particles in the alloys play a major role in passivity. Temperature?accelerates the corrosion and the higher velocity breakdown of the passive film. It also affects the resistivity of the?alloys. The results from this study also indicate that the temperature and velocity increase the negative corrosion?rate of the alloys due to higher rate of chemical reactions. SEM and EDX analysis indicate that the surfaces?compose with a thin layer of aluminum oxide and hydroxide corrosion products.
机译:这项研究的主要重点是检查和评估Fe,Ni和Cr对过共晶Al-Si汽车合金在3.5%NaCl溶液中的腐蚀行为的影响。通过在不同溶液温度和速度下进行常规的重量测量,并辅以电阻率,光学显微照片,扫描电子显微镜(SEM)和X射线分析仪(EDX)进行研究,可获得实验信息。由于在表面形成了非常薄的氧化铝和氢氧化铝薄膜,所有合金均显示出负腐蚀速率。合金中的金属间颗粒在钝化中起主要作用。温度加快了钝化膜的腐蚀和更高的速度击穿。它还会影响合金的电阻率。这项研究的结果还表明,由于较高的化学反应速率,温度和速度会增加合金的负腐蚀速率。 SEM和EDX分析表明,这些表面由一层薄薄的氧化铝和氢氧化物腐蚀产物组成。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号