Initial Ride Quality of Hot-Mix Asphalt Pavements

机译:热拌沥青路面的初始骑乘质量

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

Ride quality assessed with an inertial profiler on flexible pavement was used to provide initial information on the following key issues: repeatability associated with international roughness index (IRI) values for a wide range of hot-mix asphalt (HMA) material variables, timing of acceptance testing for initial ride quality, IRI changes with type of roadway, influence of stops and starts in the paving operation on ride quality, identification of "bump," and effect of grinding on IRI. IRI was calculated for 25-ft intervals instead of the standard 0.1 mi (528 ft) for all testing to highlight local anomalies such as bumps due to paving stoppages. Results indicate that the standard deviation of three replicate passes with an inertial profiler is 5 in./mi (includes 46 HMA mixes on the Auburn University National Center for Asphalt Technology test track). IRI measurements with time suggest that initial acceptance testing can be conducted within 7 days, which allows more flexibility in scheduling by the agency. Limited traffic also slightly reduces the IRI values, which is to the contractor's advantage. IRI values are suggested for two-lane county roads and medium- to high-traffic facilities. Separate IRI ranges are indicated for each of these categories on the basis of the type of HMA construction: new, repair and overlay, and mill and overlay. These ranges are set for best and good practices (continuous paving, no stoppages; consistent supply of trucks, very short stops). IRI values greater than 125 in./mi in any given 25-ft interval indicate a bump; bumps can be ground so that these areas have IRI values of less than 100 in./mi.
机译:使用惯性轮廓仪对柔性路面进行的骑行质量评估可提供有关以下关键问题的初步信息:与广泛的热拌沥青(HMA)材料变量相关的国际粗糙度指数(IRI)值相关的可重复性,验收时间测试初始行驶质量,IRI随巷道类型的变化,摊铺操作的起止点对行驶质量的影响,“颠簸”的识别以及磨削对IRI的影响。在所有测试中,IRI的计算间隔均为25英尺,而不是标准的0.1英里(528英尺),以突出显示局部异常,例如由于铺路停工引起的颠簸。结果表明,使用惯性分析仪进行的三遍重复试验的标准偏差为5 in./mi(包括奥本大学国家沥青技术中心测试道上的46种HMA混合物)。 IRI随时间的测量结果表明,可以在7天内进行初始验收测试,这可以使该机构在安排日程时更加灵活。有限的流量也会略微降低IRI值,这对承包商有利。建议将IRI值用于两车道的县道和中高客流量的设施。根据HMA结构的类型,为每个类别分别指定了IRI范围:新建,维修和覆盖,铣削和覆盖。这些范围是为最佳和良好做法而设置的(连续摊铺,无停顿,卡车供应稳定,停车时间非常短)。在任何给定的25英尺间隔内,IRI值均大于125 in./mi表示发生颠簸;可以对凸块进行打磨,以使这些区域的IRI值小于100 in./mi。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号