This study investigates the potential alkali silica reaction (ASR) of ferronickel slag (FNS) aggregate, which is a by-product of nickel production. A class F fly ash was used as a possible ASR mitigation in accelerated mortar bar test (AMBT) specimens containing 50% FNS. There were visible surface cracks on the specimens using no fly ash or 10% fly ash. Use of 20% fly ash reduced expansion by 45% as compared to that with 10% fly ash. In accordance with the expansion limits of Australian Standard, the mixtures using 20 and 30% fly ash were categorized as slowly reactive and nonreactive, respectively. Thermogravimetric analysis (TGA) and microstructural observations confirmed the effectiveness of fly ash in reducing Portlandite content that reduced the ASR expansion. Therefore, the use of 20-30% fly ash as cement replacement is considered as an adequate ASR mitigating measure of FNS fine aggregate.
机译:这项研究调查了镍生产副产品镍铁矿渣(FNS)骨料的潜在碱硅石反应(ASR)。在含50%FNS的加速砂浆棒试验(AMBT)标本中,使用F类粉煤灰作为缓解ASR的方法。不使用粉煤灰或10%粉煤灰的试样表面可见裂纹。与10%的粉煤灰相比,使用20%的粉煤灰可将膨胀率降低45%。根据澳大利亚标准的膨胀极限,使用20%和30%粉煤灰的混合物分别分类为慢反应性和非反应性。热重分析(TGA)和微结构观察证实了粉煤灰在减少减少ASR膨胀的硅酸盐含量方面的有效性。因此,使用20%至30%的粉煤灰替代水泥被视为FNS细骨料的ASR缓解措施。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号