首页> 外国专利> Inorganic binder for rehabilitation of gypsum-containing masonry, comprises Portland cement clinker, slag sand, brown coal fly ash or hard coal fly ash, silica fume, and stimulator of alkali carbonate, alkali hydroxide and alkali silicate

Inorganic binder for rehabilitation of gypsum-containing masonry, comprises Portland cement clinker, slag sand, brown coal fly ash or hard coal fly ash, silica fume, and stimulator of alkali carbonate, alkali hydroxide and alkali silicate

机译:用于修复含石膏砌块的无机粘合剂,包括波特兰水泥熟料,矿渣砂,褐煤粉煤灰或硬煤粉煤灰,硅粉,碱金属碳酸盐,碱金属氢氧化物和碱金属硅酸盐的刺激剂

摘要

The inorganic binder comprises Portland cement clinker (5 mass%), slag sand (20 mass%), 10-80 mass% of brown coal fly ash or hard coal fly ash, silica fume (10-80 mass%), and stimulator of alkali carbonate, alkali hydroxide, alkali silicate and alkali silicate hydrate. The binder has high stability against a reaction with calcium sulfate to thaumasite and ettringite. During hardening the binder, calcium-poor calcium silicate hydrate phase forms with a calcium/silicon ratio of 0.8-1.2. The binder is free of calcium hydroxide, calcium sulfate dihydrate, calcium sulfate and calcium oxide.
机译:无机粘合剂包括波特兰水泥熟料(5质量%),矿渣砂(20质量%),褐煤粉煤灰或硬煤粉煤灰10-80质量%,硅粉(10-80质量%)和硅酸盐的刺激剂。碱金属碳酸盐,碱金属氢氧化物,碱金属硅酸盐和碱金属硅酸盐水合物。该粘合剂对与硫酸钙反应成硅藻土和钙矾石具有高稳定性。在硬化粘合剂期间,形成钙/硅比率为0.8-1.2的贫钙硅酸钙水合物相。粘合剂不含氢氧化钙,二水合硫酸钙,硫酸钙和氧化钙。

著录项

  • 公开/公告号DE102009024200B3

    专利类型

  • 公开/公告日2010-09-30

    原文格式PDF

  • 申请/专利权人 BAUHAUS UNIVERSITAET WEIMAR;

    申请/专利号DE20091024200

  • 发明设计人 BELLMANN FRANK;STARK JOCHEN;

    申请日2009-06-08

  • 分类号C04B28/04;C04B18/14;C04B18/08;C04B14/04;

  • 国家 DE

  • 入库时间 2022-08-21 18:28:20

相似文献

  • 专利
  • 外文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号