Torrefaction of woody biomass (Acacia nilotica): Investigation of fuel and flow properties to study its suitability as a good quality solid fuel

机译:木质生物量(金合欢Nilotica)的烘焙方法:研究燃料和流动性能,以研究其适用性的优质固体燃料

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

Torrefaction of Acacia nilotica was carried out in a quartz fixed-bed reactor. Temperature and residence time varied from 220 to 280 degrees C and 20-60 min. The fuel (volatile ignitability (VI), combustibility index (CI), fuel ratio (FR)), and flow (Hausner ratio (HR), cohesion coefficient (C), Carr compressibility index (CCI), angle of repose) properties were investigated for raw and torrefled biomass. Torrefled biomass was also characterized through TGA, FTIR, SEM-EDX and ICP-MS analysis. For moisture sorption test, contact angle was measured. Finally, torrefled biomass was compared with coal using published literature. The HHV, fixed carbon content, FR of raw biomass at 280 degrees C for 40 min was increased from 19.31 to 24.76 MJ/kg, 11.35 to 60.40 wt %, and 0.13 to 1.63, respectively. While, VI, CI, C, CCI and bulk density of raw biomass at similar condition of torrefaction decreased from 15.76 to 15.37 (MJ/kg), 147.40 to 17.37 (MJ/kg), 0.40 to 0.33, 22.85 to 15.86 and 230.82 to 172.84 (kg/m(3)), respectively. ICP-MS analysis revealed that torrefled biomass was enriched in sodium, potassium, calcium, magnesium, etc. At similar torrefaction condition, the moisture absorbed by raw and torrefled biomass was 35.44% and 6.61%, respectively. Contact angle (79.1 degrees/77.5 degrees) for torrefled biomass suggested its hydrophobic nature. (C) 2020 Elsevier Ltd. All rights reserved.
机译:在石英固定床反应器中进行了金合欢尼尔替替氏菌。温度和停留时间从220变化到280℃和20-60分钟。燃料(挥发性可燃性(VI),可燃指数(CI),燃料比(FR)和流量(Hausner比(HR),内聚力系数(C),Carr可压缩指数(CCI),Reachose ins,Reachose)性质是调查原料和烘焙生物量。 Torrefled BioMass的特征还通过TGA,FTIR,SEM EDX和ICP-MS分析。对于水分吸附试验,测量接触角。最后,使用公开的文献将Torrefled BioMass与煤进行比较。 HHV,固定碳含量,在280℃下的原料生物量的Fr,从19.31增加到24.76mJ / kg,11.35至60.40wt%,分别为0.13至1.63。虽然在类似烘焙状况下的原料生物量的VI,CI,C,CCI和堆积密度从15.76到15.37(MJ / kg),147.40至17.37(MJ / kg),0.40至0.33,22.85至15.86和230.82分别为172.84(kg / m(3))。 ICP-MS分析表明,在类似的烘焙状况下富含钠,钾,钙,镁等的酸丁杂化生物质,通过原料和烘焙生物量吸收的水分分别为35.44%和6.61%。 Torrefled Biomass的接触角(79.1度/ 77.5度)表明其疏水性质。 (c)2020 elestvier有限公司保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号