Spent fuel rod splitting due to UO_2 oxidation during dry storage: Assessment of the database

机译:干储存过程中由于UO_2氧化而导致的燃料棒破损:数据库评估

获取原文
获取原文并翻译 | 示例
       

摘要

Dry interim storage is becoming a common practice worldwide. The potential contact between "undamaged" (i.e., not detected as damaged, but containing tiny defects like pinholes and hairline cracks) fuel rods and an oxidizing atmosphere during the cask water removal might lead to unacceptable consequences. One way to prevent it is to determine the time to propagation of a defect at given conditions.rnThis paper compiles and critically reviews the existing database concerning time-at-temperature profile of fuel rods containing tiny defects (i.e., pinholes and hairline cracks) that are exposed to oxidizing atmospheres. Temperature and burnup have been identified as the main variables influencing the incubation time under the conditions explored by the experiments carried out. By correlating all the experimental data gathered, an empirical correlation of an Arrhenius-type has been derived that encapsulates the temperature and burnup effects in a satisfactory way (i.e., relative error less than 36% and R~2 = 0.87). Additionally, the sensitivity of time-to-propagation to changes in both variables has been investigated. The major database weaknesses are data scarcity and test boundary conditions far away from the ones shown by the spent fuel discharged from reactors nowadays (i.e., too low burnup or unlimited flow of oxidizing agent). Based on them, a proposal for further investigation is proposed to make time-at-temperature profiles a sound and reliable tool to assess the effect of potential fuel oxidation on "undamaged" fuel rods integrity.
机译:干式临时存储已成为全球通用的做法。去除桶装水期间,“未损坏”(即未检测到损坏,但包含细小缺陷(如针孔和细线裂纹)之类的燃料棒与氧化性气氛之间的潜在接触可能会导致无法接受的后果。防止这种情况的一种方法是确定在给定条件下缺陷的传播时间。rn本文汇总并严格审查了有关包含微小缺陷(例如,针孔和细线裂纹)的燃料棒的温度时间曲线的现有数据库。暴露在氧化气氛中。在进行的实验探索的条件下,温度和燃耗已被确定为影响孵育时间的主要变量。通过关联所有收集的实验数据,得出了Arrhenius型的经验关联,该关联以令人满意的方式封装了温度和燃耗效应(即,相对误差小于36%,R〜2 = 0.87)。另外,已经研究了传播时间对两个变量的变化的敏感性。数据库的主要弱点是数据稀缺性和测试边界条件,这些条件与当今反应堆排出的乏燃料所显示的条件相去甚远(即燃尽率太低或氧化剂流量无限大)。在此基础上,提出了进一步研究的建议,以使温度变化时间曲线成为评估潜在燃料氧化对“未损坏”燃料棒完整性的影响的可靠且可靠的工具。

著录项

  • 来源
    《Progress in nuclear engergy》 |2009年第2期|201-206|共6页
  • 作者

    L.E. Herranz; F. Feria;

  • 作者单位

    Unit of Nuclear Safety Research (CIEMAT), Avda. Complutense, 22 - 28040 Madrid, Spain;

    Unit of Nuclear Safety Research (CIEMAT), Avda. Complutense, 22 - 28040 Madrid, Spain;

  • 收录信息 美国《科学引文索引》(SCI);美国《工程索引》(EI);
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    rod splitting; UO_2 oxidation; dry storage;

    机译:杆劈;UO_2氧化;干燥储存;
  • 入库时间 2022-08-18 00:43:48

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号