Thermogravimetric analysis of compatibilized blends of low density polyethylene and poly(dimethyl siloxane) rubber

机译:低密度聚乙烯和聚二甲基硅氧烷橡胶相容混合物的热重分析

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

The thermogravimetric (TG) and derivative thermogravimetric (DTG) analysis of compatibilized blends of low density polyethylene (LDPE) and poly(dimethyl siloxane) rubber (PDMS) in the proportion of 50:50 containing different proportions of ethylene methyl acrylate co-polymer (EMA) as compatibilizer have been studied. EMA acts as a chemical polymeric compatibilizer for the binary blend system of LDPE and PDMS, the proportion of which varied from 0 to 15 wt.%. The TG and DTG of the blends show that the thermal degradation takes place in two stages, where as neat LDPE shows a three stage degradation and neat EMA and PDMS show only single stage degradations respectively. The activation energies at 10% degradation have been determined using Freeman and Carroll's method and found to be maximum (171 kJ/mol) for the blend containing 6 wt.% of EMA. Half life periods at 200 degreesC have been evaluated by the Flynn and Wall method and found to be maximum for the blend containing 6 wt.% of EMA. (C) 2003 Published by Elsevier Science Ltd. [References: 15]
机译:低密度聚乙烯(LDPE)和聚(二甲基硅氧烷)橡胶(PDMS)以50:50的比例包含不同比例的乙烯丙烯酸甲酯共​​聚物的增容共混物的热重(TG)和导数热重(DTG)分析( EMA)作为增容剂已被研究。 EMA充当LDPE和PDMS的二元共混体系的化学聚合物增容剂,其比例在0至15 wt。%之间变化。共混物的TG和DTG显示热降解发生在两个阶段,其中纯LDPE显示三阶段降解,而纯EMA和PDMS分别仅显示单阶段降解。使用Freeman和Carroll的方法测定了降解10%时的活化能,发现对于含有6 wt。%EMA的共混物,活化能最大(171 kJ / mol)。已经通过Flynn和Wall方法评估了在200℃下的半衰期,并且发现其对于含有6重量%的EMA的共混物是最大的。 (C)2003年由Elsevier Science Ltd.出版[参考文献:15]

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号