The thermal oxidation of unstabilised polypropylene (PP) was studied at 80 degrees C under various oxygen pressures: 0.02, 0.5 and 5.0 MPa, and, under 5.0 MPa oxygen pressure at various temperatures: 60, 80, 100 and 120 degrees C. Hydroperoxides were titrated using a chemical titration method and modulated DSC (taking an enthalpy of -325 kJ mol(-1)). Starting from a previous kinetic analysis of carbonyl growth in same exposure conditions, we have tried to simulate experimental results by a model based on the classical mechanistic scheme in which initiation results from POOH (mainly bimolecular) decomposition. The model, which takes into account substrate consumption and does not rely on usual simplifying assumptions (steady state for radicals, long kinetic chains, interrelations between termination rate constants), generates kinetic curves with the same shape as experimental ones and predicts well the effect of O-2 pressure and temperature on hydroperoxide and carbonyl concentrations. (c) 2006 Elsevier Ltd. All rights reserved.
机译:研究了不稳定的聚丙烯(PP)在80摄氏度,各种氧气压力:0.02、0.5和5.0 MPa下的热氧化,以及在5.0 MPa氧气压力下在60、80、100和120摄氏度的各种温度下的热氧化。使用化学滴定法和调制的DSC滴定法(焓为-325 kJ mol(-1))。从先前在相同暴露条件下羰基生长的动力学分析开始,我们尝试通过基于经典机理方案的模型来模拟实验结果,其中经典机理是由POOH(主要是双分子)分解引发的。该模型考虑了底物消耗,并且不依赖于通常的简化假设(自由基的稳态,长的动力学链,终止速率常数之间的相互关系),生成的动力学曲线与实验形状相同,并很好地预测了O-2的压力和温度对过氧化氢和羰基浓度的影响。 (c)2006 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号