Boric acid supported natural rubber (BSNR) was prepared from the reaction between hydroxyl group in diol functionalized natural rubber and boric acid. The optimum condition was assessed by the influences of different boric acid concentrations used in a term of [boric acid]/[diol unit] molar ratio and reaction time. The increase of them led to increasing the participation of boric acid into the rubber molecules, which was structural as boronic acid unit in BSNR. The determination of boron element quantity of BSNRs was found to increase with increasing mole% of boron containing rubber. Furthermore, the increase of mole% of boron content caused the increase of Mooney viscosity, glass transition temperature (T_g), thermal stability and improving flammability behaviors by the reduction of HRR_(max), THR, EHC, MRL CO_2 and burning rate as well as the increase of LOI values over original epoxidized natural rubber (ENR).
机译:由二醇官能化天然橡胶中的羟基与硼酸之间的反应制备了硼酸负载天然橡胶(BSNR)。通过以[硼酸] / [二醇单元]摩尔比和反应时间的术语使用的不同硼酸浓度的影响来评估最佳条件。它们的增加导致硼酸对橡胶分子的参与增加,其在BSNR中以硼酸单元的形式存在。发现BSNRs的硼元素含量的测定随含硼橡胶的摩尔%的增加而增加。此外,硼含量摩尔%的增加还导致门尼粘度,玻璃化转变温度(T_g),热稳定性的提高,并通过降低HRR_(max),THR,EHC,MRL CO_2和燃烧速率来改善可燃性。与LOI值相比,原始环氧化天然橡胶(ENR)有所增加。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号