In the present work, the flammability of Kyowaglas is characterized experimentally. Kyowaglas is a lead-based composite used in glove boxes of nuclear facilities as a biological protection against radiation. It consists of 70%_(wt) PMMA (Poly(Methyl Methacrylate)) and 30%_(wt) leaded compounds. The aim of the study is to understand the role and impact of lead during the combustion of Kyowaglas in order to deepen knowledge of its thermal and fire behavior. A comparative study between Kyowaglas and virgin PMMA is conducted to better understand the effect of lead on the combustion process of these materials. Fire behavior is studied using cone calorimeter, pyrolysis-combustion flow calorimeter and thermogravimet-ric analysis. At different stages of cone calorimeter test, the samples and residues were examined and characterized using different experimental techniques like microscopy, spectroscopy, X-ray diffraction and calorimetry. Thermal analysis data show that lead seems to slightly accelerate the decomposition of PMMA under inert atmosphere. However, it confers significant thermal stability during a cone test due to the accumulation of lead on the surface of the sample. As the Kyowaglas burns, metallic lead is formed and accumulated at the top surface slowing down the heat transfer. At the end of the cone calorimeter test, lead oxide beads start to form on the surface of the residue due to the oxidation of metallic lead.
机译:在目前的工作中,KyowAglas的可燃性在实验上表征。 Kyowaglas是一种用于核设施手套盒的铅基复合材料,作为防辐射的生物保护。它由70%_(WT)PMMA(聚(甲基丙烯酸甲酯))和30%_(WT)铅化合物组成。该研究的目的是了解在Kyowaglas燃烧过程中铅的作用和影响,以加深其热和火灾行为的知识。进行KyowAglas和Virgin PMMA之间的比较研究,以更好地了解铅对这些材料的燃烧过程的影响。使用锥形量热计,热解 - 燃烧流量热计和热重度分析研究了防火行为。在锥形量热计试验的不同阶段,使用不同的实验技术,如显微镜,光谱,X射线衍射和量热法,检查样品和残留物。热分析数据显示,铅似乎略微加速PMMA在惰性气氛下的分解。然而,由于样品表面上的铅积累,它在锥形测试期间赋予显着的热稳定性。作为kyowaglas烧伤,金属铅形成并积聚在顶部表面上减慢传热。在锥形量热计测试结束时,由于金属铅的氧化,氧化铅珠子开始在残留物的表面上形成。

著录项

  • 来源
    《Polymer Degradation and Stability》 |2021年第8期|109618.1-109618.17|共17页
  • 作者单位

    Institut de Radioprotection et de Surete Nucleaire (IRSN) PSN-RES/SA2I Cadarache Saint-Paul-Lez-Durance 13115 France;

    IMT - Mines Ales Polymers Hybrids and Composites (PCH) 6 Avenue De Clavieres Ales Cedex F-30319 France;

    IMT - Mines Ales Polymers Hybrids and Composites (PCH) 6 Avenue De Clavieres Ales Cedex F-30319 France;

    Institut de Radioprotection et de Surete Nucleaire (IRSN) PSN-RES/SA2I Cadarache Saint-Paul-Lez-Durance 13115 France;

  • 收录信息
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    Kyowaglas; PMMA; Lead; Lead oxide; Thermal stability;

    机译:kyowaglas;PMMA;带领;氧化铅;热稳定性;

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号