The purpose of this study was to determine the effect of addition of by products from seaweed industry as a sand complement material on the manufacture of lightweight concrete(CLC). This research was experimental studied by making lightweight concrete CLC depends on different concentration of complement by products seaweed industry and sand (0%: 100%; 10%: 90%; 20%: 80%; 30%: 70%; 40%: 60%; 50%: 50. The lightweight concrete quality assay that used on this study was compressive strength, splitting tensile strength, density, and water absorption. The highest compressive strength of lightweight concrete by concentration 50% of addition industrial seaweed byproducts with a large 1,21 Mpa. The highest splitting tensile strength was found on the addition of 50% seaweed industrial byproducts with a large 0.122 MPa. The biggest of water absorption of lightweight concrete was found on addittion 50% of industrial seaweed byproducts by 55.25%, While, the highest density was found on the addition of byproducts with a concentration 50 % by 0.87 kg/L.
机译:本研究的目的是确定通过海藻工业的产品加入的效果作为制造轻质混凝土(CLC)的砂补充材料。该研究是通过制造轻量级混凝土CLC研究的实验性,这取决于产品海藻行业和沙子的不同浓度(0%:100%; 10%:90%:80%; 80%; 30%:70%:40%: 60%; 50%:50。用于本研究的轻质混凝土质量测定是抗压强度,分裂拉伸强度,密度和吸水性。轻量级混凝土的最高抗压强度由浓度为50%的加入工业海藻副产品大1,21个MPa。在加入50%的海藻工业副产物中,具有大0.122MPa的加入最高分裂拉伸强度。在55.25%的工业海藻副产品中发现了轻质混凝土的最大吸水性。虽然,在添加浓度为50%(0.87kg / L的副产物上)发现最高密度。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号