Pine wood (Pinus sylvestris) was delignified using a modern displacement kraft cooking method. A series of laboratory-scale cooks ("stop-cooks") was carried out to different cooking degrees representing i) the end points of "warm black liquor impregnation" (temperature 80℃, total yield 93.3%) and "hot black liquor pretreatment" (temperature 155℃, total yield 77.5%) and ii) varying chlorine numbers (1.8-7.0) in the cooking stage (temperature 170℃, H factor 370-1820, total yield 40.7-48.6%). The resulting black liquors were analysed in terms of carbohydrate-derived aliphatic carboxylic acids and the fraction of lignin degradation products including its molecular mass distribution. Total yield, residual lignin content, viscosity and brightness were determined from the corresponding pulps. Based on these results the dissolution of different wood carbohydrates and lignin was monitored as a function of total yield. The chemical stability of lignin material in black liquor was studied separately by treating the corresponding liquor at temperatures of 160℃ and 175℃ for 15-480 minutes. At both temperatures a slight degradation of lignin was detected during the treatment.
机译:松木(Pinus sylvestris)使用现代置换牛皮纸蒸煮方法进行脱木质处理。进行了一系列实验室规模的烹饪(“停止烹饪”),以不同的烹饪度来表示:i)“温热黑液浸渍”(温度80℃,总产率93.3%)和“热黑液预处理”的终点”(温度155℃,总产率77.5%)和ii)在蒸煮阶段(温度170℃,H因子370- 1820,总产率40.7-48.6%)改变氯含量(1.8-7.0)。根据碳水化合物衍生的脂肪族羧酸和木质素降解产物的分数(包括其分子量分布)对所得黑液进行了分析。从相应的纸浆确定总产率,残余木质素含量,粘度和亮度。基于这些结果,监测了不同木材碳水化合物和木质素的溶出度与总产量的关系。通过在160℃和175℃分别处理15-480分钟,分别研究木质素原料在黑液中的化学稳定性。在两个温度下,在处理过程中都检测到木质素的轻微降解。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号