Elevated temperature tensile and creep-rupture tests were performed on INCONEL alloy MA754 in an as-rolled, fine-grained condition. Tensile tests were performed at 25 °C, 800 °C, 900 °C, and 1000 °C; creep-rupture tests were performed at 800 °C, 900 °C, and 1000 °C. the elevated temperature strength in the fine-grained condition was approximately 25 pct of that the coarse-grained, annealed condition. While good ductility was observed in tensile tests at a nominal strain rate of 1 × 10−3s−1, ductility in creep-rupture tests was very low, with failure elongations less than 5 pct and no reduction in area. Creep deformation appeared to occur primarily by cavity formation and growth.
机译:在轧制的细晶粒条件下,对INCONEL合金MA754进行了高温拉伸和蠕变断裂测试。在25°C,800°C,900°C和1000°C下进行拉伸测试;蠕变断裂试验在800°C,900°C和1000°C下进行。在细颗粒状态下的高温强度约为粗颗粒退火状态下的25%。虽然在名义应变率为1×10−3 s−1 的拉伸试验中观察到良好的延展性,但蠕变断裂试验的延展性非常低,破坏伸长率小于5 pct,没有减少面积。蠕变变形似乎主要是由于空腔的形成和生长而发生的。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号