A comparison of shear instability in U-Ti vs W alloy-during high strain rate deformation is resented. Experimental quasi-static and dynamic deformation data are used to formulate the constitutive description based on the mechanical threshold stress model (MTS). The MTS model is used to predict the deformation behavior of U-Ti and W-alloy beyond the conventionally achievable experimental capabilities. We suggest that uranium alloys are more prone to catastrophic-localized deformation (adiabatic shearing) due to the existence of a soft high-temperature phase, which is reached by uranium alloys undergoing large strains at high strain rate of deformation.
机译:比较了U-Ti和W合金在高应变率变形过程中的剪切不稳定性。实验准静态和动态变形数据用于基于机械阈值应力模型(MTS)建立本构描述。 MTS模型用于预测U-Ti和W合金超出常规可达到的实验能力的变形行为。我们认为,由于存在软的高温相,铀合金更容易发生灾难性的局部变形(绝热剪切),这是由于铀合金在高应变率下承受大应变而达到的。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号