Magnesium substituted low crystalline beta-tricalcium phosphates (LC-beta-TCP) is an attractive biomaterials owing to its high initial osteoconductivity and bone regeneration. The present investigation is focused on fabrication of low crystalline beta-TCP (LC-beta-TCP) and evaluating in vitro dissolution toward to the crystallinity of the LC-beta-TCP. It is suggested that the crystallinity of biocompatible ceramics greatly affect into their biocompatibility. The novelty of the work is the preparation of the LC-beta-TCP without any calcium carbonate/phosphate complex, which is commonly in use. LC-beta-TCP was fabricated from MgHPO4 center dot 3H(2)O (MgP) and CaCl2 aqueous solution at 200 degrees C hydrothermal condition. In vitro dissolution evaluations simulated osteoclast condition indicated the release of Mg2+ and Ca2+. It is suggested that LC-beta-TCP fabricated by the given method could be useful material for bone regeneration because it has both low crystallinity and suitable Ca2+ and Mg2+ releasing and most importantly it does not contain any extended protocol.
机译:镁取代的低结晶β-三钙磷酸酯(LC-β-TCP)是一种有吸引力的生物材料,因为它具有很高的初始骨传导性和骨骼再生能力。本研究的重点是低结晶β-TCP(LC-β-TCP)的制造,并评估LC-β-TCP结晶度的体外溶出度。建议生物相容性陶瓷的结晶度极大地影响其生物相容性。这项工作的新颖之处在于制备了不使用任何碳酸钙/磷酸盐复合物的LC-β-TCP,这是通常使用的。 LC-beta-TCP由MgHPO4中心点3H(2)O(MgP)和CaCl2水溶液在200摄氏度的水热条件下制备。体外溶出度评估模拟破骨细胞状况表明Mg2 +和Ca2 +的释放。建议通过给定方法制造的LC-β-TCP可能是骨再生的有用材料,因为它具有低结晶度和合适的Ca2 +和Mg2 +释放能力,最重要的是它不包含任何扩展协议。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号