The cast pipe joint of the Fe-15Mn-5Si-8Cr-5Ni-0.25C alloy was manufactured (the numbers in the composition denote the weight percentage of the elements while the weight percentage of Fe is the balance). The corresponding microstructure and shape memory effect are compared with those of a forged alloy. The results show that the cast joint has a good shape memory effect and may be industrially applied while the cast joint keeps jointing under a tensile force of 20 kN and a sealing pressure of 5 MPa. Moreover, it is found that the addition of nitrogen in the alloy doesn't evidently improve the shape memory effect of the alloy.
机译:制造Fe-15Mn-5Si-8Cr-5Ni-0.25C合金的铸管接头(组成中的数字表示元素的重量百分比,而Fe的重量百分比为余量)。将相应的显微组织和形状记忆效应与锻造合金进行比较。结果表明,该铸造接头具有良好的形状记忆效果,可在工业上应用,同时该铸造接头在20 kN的拉力和5 MPa的密封压力下保持接合。此外,发现在合金中添加氮并不能明显改善合金的形状记忆效果。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号