PURPOSE:To form the joint without any welding defect by thinning the welding zone of the Al die cast member to be overlapped on the surface of the welding zone of Al alloy cast member toward the tip, by cutting off the tip nearly vertically and by directing an arc for the position slightly apart from the tip. CONSTITUTION:The welding part of the Al alloy die cast member 20 to be joined with welding to Al alloy cast member 1 is made in the following shape: the face 28, etc. inclining to a mating surface 9 are provided and thinned toward the tip; the tip face 27 is formed in the gapping shape about vertically for the mating surface 9 further. A welding wire 31, namely, an arc is welded toward the mating surface 9 with slightly separating from the tip face 27. The thermal capacity of the welding part of the member 20 is thus reduced and the welding part of the die cast member 20 can be welded with less heat gain and penetration even in case of the penetration at the cast member 1 side being made much sufficiently. Accordingly the generation of blow hole is controlled and the welding zone without defect is obtd.
机译:目的:通过变薄铝压铸件的焊接区域,使其重叠在铝合金铸件的焊接区域的表面上,朝焊嘴方向倾斜,形成接缝,方法是将焊嘴几乎垂直地切掉并定向与尖端稍微分开的位置的弧线。组成:铝合金压铸件20的焊接部分将与铝合金压铸件1焊接在一起,其形状如下:提供倾斜到配合面9的面28等,并朝尖端变薄;端面27进一步形成为与配合面9大致垂直的间隙形状。焊丝31,即电弧,以与尖端表面27稍微分离的方式朝向配合面9焊接。因此,降低了构件20的焊接部分的热容量,并且压铸构件20的焊接部分可以即使在铸造构件1侧的熔深足够大的情况下,也能够以较少的热量获得和熔深进行焊接。因此,控制了气孔的产生,并且消除了无缺陷的焊接区域。

著录项

  • 公开/公告号JPH0370585B2

    专利类型

  • 公开/公告日1991-11-08

    原文格式PDF

  • 申请/专利权人 DAIHATSU MOTOR CO LTD;

    申请/专利号JP19850171599

  • 发明设计人 OOBA YASUSHI;TANAKA YUTAKA;

    申请日1985-08-02

  • 分类号B23K9/23;

  • 国家 JP

  • 入库时间 2022-08-22 06:01:36

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号