首页> 外文期刊>Materials & design >A study on fracture behaviour of three different high strength low alloy steel sheets during formation with different strain ratios
【24h】

A study on fracture behaviour of three different high strength low alloy steel sheets during formation with different strain ratios

机译:不同应变比的三种不同高强度低合金钢板成形过程中的断裂行为研究

获取原文
获取原文并翻译 | 示例

摘要

This paper deals with the study on fracture behaviour of three different steels, namely, the HSLA, the Micro alloyed and the Carbon-Manganese steels, using stress- and strain-based forming and fracture limit diagrams obtained from the experimentally determined strain values for different strain or stress ratios. With an aim to analyse the fracture behaviour, the strain- and stress-based forming and fracture limit diagrams have been developed for three different steel sheets, namely, the HSLA steel sheet of 1.6 mm thickness, the Micro alloyed steel sheet of 1.2 mm thickness, and the Carbon-Manganese steel sheet of 1.4 mm thickness. The forming and fracture behaviour and size and shape of voids (particularly, the ratio of length to width of voids, (L/W)) developed at fracture during the formation of these steels, under different strain ratio conditions, have been correlated with the mechanical properties such as microstructure of steels, minor strain at fracture, and Mohr's circle shear strains, various combinations of mean strain and effective strain, and material properties, namely, strain hardening exponent (n)-value, normal anisotropy (r) and the range of localized neckings.
机译:本文使用基于应力和应变的成形以及从实验确定的不同应变值获得的断裂极限图,研究了三种不同钢(HSLA,微合金钢和碳锰钢)的断裂行为。应变或应力比。为了分析断裂行为,已针对三种不同的钢板(基于1.6毫米厚的HSLA钢板,1.2毫米厚的微合金钢板)绘制了基于应变和应力的成形和断裂极限图。 ,以及厚度为1.4毫米的碳锰钢板。在不同应变比条件下,这些钢在断裂过程中形成时的断裂行为,空隙的大小和形状(特别是空隙的长宽比(L / W))与钢的断裂强度相关。力学性能,例如钢的微观结构,断裂时的小应变和莫尔圆剪切应变,平均应变和有效应变的各种组合以及材料特性,例如应变硬化指数(n)值,法向各向异性(r)和局部颈缩的范围。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号