Failure of the bond between the acrylic resin and resilient liner material is commonly encountered in clinical practice. The purpose of this study was to investigate the effect of different surface treatments (sandblasting, Er:YAG, Nd:YAG, and KTP lasers) on tensile bond strength of silicone-based soft denture liner. Polymethyl methacrylate test specimens were fabricated and each received one of eight surface treatments: untreated (control), sandblasted, Er:YAG laser irradiated, sandblasted + Er:YAG laser irradiated, Nd:YAG laser irradiated, sandblasted + Nd:YAG laser irradiated, KTP laser irradiated, and sandblasted + KTP laser irradiated. The resilient liner specimens (n = 15) were processed between two polymethyl methacrylate (PMMA) blocks. Bonding strength of the liners to PMMA were compared by tensile test with the use of a universal testing machine at a crosshead speed of 5 mm/min. Kruskal–Wallis and Wilcoxon tests were used to analyze the data (α = 0.05). Altering the polymethyl methacrylate surface by Er:YAG laser significantly increased the bond strengths in polymethyl methacrylate/silicone specimens, however, sandblasting before applying a lining material had a weakening effect on the bond. In addition, Nd:YAG and KTP lasers were found to be ineffective for increasing the strength of the bond.
机译:在临床实践中,丙烯酸树脂和弹性衬里材料之间的粘结失效是常见的。这项研究的目的是研究不同表面处理(喷砂,Er:YAG,Nd:YAG和KTP激光)对有机硅基假牙衬里抗拉强度的影响。制作了聚甲基丙烯酸甲酯测试样品,并分别进行了以下八个表面处理之一:未处理(对照),喷砂,Er:YAG激光辐照,喷砂+ Er:YAG激光辐照,Nd:YAG激光辐照,喷砂+ Nd:YAG激光辐照,照射KTP激光,并喷砂+ KTP激光。在两个聚甲基丙烯酸甲酯(PMMA)块之间处理了弹性衬里样品(n = 15)。衬里与PMMA的结合强度通过拉伸测试与万能测试机以5 mm / min的十字头速度进行了比较。使用Kruskal–Wallis和Wilcoxon检验分析数据(α= 0.05)。用Er:YAG激光改变聚甲基丙烯酸甲酯的表面可以显着提高聚甲基丙烯酸甲酯/硅树脂样品的结合强度,但是,在应用衬里材料前进行喷砂处理对结合力的影响较小。此外,发现Nd:YAG和KTP激光器对于增加粘结强度无效。

著录项

  • 来源
    《Lasers in Medical Science》 |2011年第6期|p.783-788|共6页
  • 作者单位

    Department of Prosthodontics, Faculty of Dentistry, University of Cumhuriyet, 58140, Sivas, Turkey;

    Department of Prosthodontics, Faculty of Dentistry, University of Cumhuriyet, 58140, Sivas, Turkey;

    Department of Prosthodontics, Faculty of Dentistry, University of Cumhuriyet, 58140, Sivas, Turkey;

    Department of Conservative Dentistry, Faculty of Dentistry, University of Cumhuriyet, 58140, Sivas, Turkey;

    Department of Prosthodontics, Faculty of Dentistry, University of Cumhuriyet, 58140, Sivas, Turkey;

  • 收录信息
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    Er:YAG laser; Nd:YAG laser; KTP laser; Sandblasting; Tensile bond strength; Soft denture liner;

    机译:Er:YAG激光;Nd:YAG激光;KTP激光;喷砂;拉伸粘结强度;软义齿衬里;

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号