The tensile behavior of quasi-isotropic woven silicon carbide fabric reinforced silicon-carbon-nitrogen (SiC/SiNC) matrix composites has been investigated at both room and elevated temperature. The load-displacement and subsequent stress- strain curves at a temperature range of 230 deg C-13800 deg C were generated. The failure strength, failure strain. proportional limit and modulus of SiC/SiNC composites are reported. The failure mechamsms under monotonic tensile loading were studied using acoustic emission techinque and detailed optical and scanning electron microscopic examinations. The SiC/SiNC woven composites were analyzed under tensile loading by finite element method using isoparanietric layered shell elements. The thermal stresses at different temperature range are also incorporated with the mechanical stress in order to observe the influence of thermal expansion coefficient at elevated temperature. Both the normal and interlaminar shear stress distribution across the thickness are analyzed at room and elevated temperatures.
机译:研究了准各向同性编织碳化硅织物增强的硅碳氮(SiC / SiNC)基复合材料在室温和高温下的拉伸性能。在230摄氏度至13800摄氏度的温度范围内生成了载荷-位移和随后的应力应变曲线。破坏强度,破坏应变。报告了SiC / SiNC复合材料的比例极限和模量。使用声发射技术以及详细的光学和扫描电子显微镜检查研究了单调拉伸载荷下的破坏机理。 SiC / SiNC机织复合材料在拉伸载荷下通过等分层状壳单元的有限元方法进行了分析。为了观察高温下热膨胀系数的影响,还将不同温度范围内的热应力与机械应力结合在一起。在室温和高温下,都可以分析整个厚度上的正向和层间剪切应力分布。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号