Stress intensity factor K is analyzed by measuring distribution of sum of the principal stresses around slit tip by an infrared stress measuring device. Under the biaxial tensile stress, both K-values of the isotropic materials with slit angle 0° and 45° show there is no influence of the slit angle at Mode Ⅰ. The tolerance of the measured K-values of the test specimens which are compared with measured K-values by photoelastic method are around 10-20% , and these increase as applied cyclic load increases. These tolerance can be reduced up to about 8% by modifying measurements. The effectiveness of the thermoelastic stress measurement method to K_I value analyzing under biaxial tensile stress was confirmed.
机译:通过利用红外应力测量装置测量狭缝尖端周围的主应力之和的分布来分析应力强度因子K。在双轴拉伸应力下,缝隙角分别为0°和45°的各向同性材料的K值都表示在模式Ⅰ下缝隙角没有影响。与通过光弹性法测量的K值相比,试样的测量的K值的公差为10-20%左右,并且随着施加的循环载荷的增加而增加。通过修改测量值,可以将这些容差降低多达8%。证实了热弹性应力测量方法对双轴拉伸应力下的K_I值分析的有效性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号