A test protocol and a data analysis method are developed in this paper on the basis of linear viscoelastic theory to characterize the anisotropic viscoelastic properties of undamaged asphalt mixtures. The test protocol includes three nondestructive tests: (1) uniaxial compressive creep test, (2) indirect tensile creep test, and (3) the uniaxial tensile creep test. All three tests are conducted on asphalt mixture specimens at three temperatures (10, 20, and 30°C) to determine the tensile and compressive properties at each temperature and then to construct the master curve of each property. The determined properties include magnitude and phase angle of the compressive complex modulus in the vertical direction, magnitude and phase angle of the tensile complex modulus, and the magnitude and phase angle of the compressive complex modulus in the horizontal plane. The test results indicate that all tested asphalt mixtures have significantly different tensile properties from compressive properties. The peak value of the master curve of the tensile complex modulus phase angle is within a range from 65 to 85°, whereas the peak value of the compressive moduli phase angle in both directions ranges from 35 to 55°. In addition, the undamaged asphalt mixtures exhibit distinctively anisotropic properties in compression. The magnitude of the compressive modulus in the vertical direction is approximately 1.2 to ~2 times of the magnitude of the compressive modulus in the horizontal plane. Dynamic modulus tests are performed to verify the results of the proposed test protocol. The test results from the proposed test protocol match well with those from the dynamic tests.
机译:在线性粘弹性理论的基础上,开发了一种测试方案和一种数据分析方法,以表征未损坏沥青混合料的各向异性粘弹性。该测试方案包括三个非破坏性测试:(1)单轴压缩蠕变测试,(2)间接拉伸蠕变测试和(3)单轴拉伸蠕变测试。所有这三个测试都是在三种温度(10、20和30°C)下对沥青混合料样品进行的,以确定每种温度下的拉伸和压缩性能,然后构建每种性能的主曲线。所确定的性质包括在垂直方向上的压缩复数模量的大小和相位角,在拉伸方向上的拉伸复数模量的大小和相位角以及在水平平面上的压缩复数模量的大小和相位角。测试结果表明,所有测试的沥青混合料均具有与压缩性能显着不同的拉伸性能。拉伸复模量相角的主曲线的峰值在65至85°的范围内,而在两个方向上的压缩模量相角的峰值在35至55°的范围内。另外,未损坏的沥青混合物在压缩时表现出明显的各向异性。垂直方向上的压缩模量的大小是水平面上的压缩模量的大小的约1.2至约2倍。执行动态模量测试以验证所提出的测试协议的结果。提议的测试协议的测试结果与动态测试的结果非常匹配。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号