The surface softness and mechanical properties of wood pulp-lyocell wet-laid nonwoven fabric

机译:木材纸浆Lyocell湿式非织造织物的表面柔性和力学性能

获取原文
获取原文并翻译 | 示例
           

摘要

This study explores the tensile properties of wet-laid nonwoven fabric made from softwood bleached kraft pulp (SwBKP), hardwood bleached kraft pulp (HwBKP), dissolving pulp (DP), and Lyocell. Five different ratios of wood pulp and Lyocell (0/100, 10/90, 20/80, 30/70, 40/60, and 50/50) were manufactured using papermaking technology, which is similar to wet-laid technology. The results indicate that the properties of strength and surface softness of a nonwoven fabric are enhanced by the contribution of the entanglements of wood pulp-Lyocell. Of the three pulps, SwBKP is superior to both HwBKP and DP on account of its higher properties of density and tensile strength, which are increased by refining treatments. In terms of the surface softness component results, HwBKP has a lower MMD value than the other samples. The SwBKP-Lyocell mixing ratios with the minimum ratio of 30/70 were found to offer sufficient tensile strength with improved softness.
机译:本研究探讨了由软木漂白牛皮纸(SWBKP),硬木漂白的牛皮浆(HWBKP),溶解纸浆(DP)和Lyocell制成的湿式非织造织物的拉伸性能。 使用造纸技术制造了五种不同的木浆和Lyocell(0/100,10 / 90,20 / 80,20 / 80,20 / 50)的比例,类似于湿式技术。 结果表明,无纺布的强度和表面柔软度的性能通过木浆-Lyocell的缠结贡献而增强。 在三个纸浆中,SWBKP由于其较高的密度和拉伸强度的性能而优于HWBKP和DP,这通过精炼处理增加。 就表面柔软性分量结果而言,HWBKP具有比其他样品更低的MMD值。 发现具有30/70的最小比例的SWBKP-Lyocell混合比率提供足够的拉伸强度,具有改善的柔软性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号