Apparent energy of activation for hot working of vanadium microalloyed steel

机译:钒微合金钢热加工的活化视在能量

获取原文
获取原文并翻译 | 示例
           

摘要

Two-stage linear ln [sinh(ασ)] vs. 1/T plots, based on isothermal continuous and anisothermal multipass torsion curves, indicate the double Q_(HW) behaviour of a V-steel. Above T_(nr), Q_(HW) is independent of all variables but strain. Below T_(nr) (which is interpass time dependent), i.e., in a temperature range in which interpass rccrystallization is supressed, Q_(HW) is not only increased but that based on multipass curves is also interpass time dependent, and only valid for multipass working operations.
机译:基于等温连续和等温多遍扭转曲线的两阶段线性ln [sinh(ασ)]与1 / T曲线表明V型钢的双重Q_(HW)性能。在T_(nr)以上,Q_(HW)与所有变量无关,但应变除外。低于T_(nr)(取决于层间时间),即在抑制层间再结晶的温度范围内,不仅增加了Q_(HW),而且基于多道次曲线的Q_(HW)也取决于层间时间,并且仅对多遍工作操作。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号