The usability of hydrogen and also carbon containing fuels is one of the important advantages of solid oxide fuel cells (SOFCs), which opens the possibility to use fuels derived from conventional sources such as natural gas and from renewable sources such as biogas. Impurities like sulfur compounds are critical in this respect. State-of-the-art Ni/YSZ SOFC anodes suffer from being rather sensitive towards sulfur impurities. In the current study, anode supported SOFCs with Ni/YSZ or Ni/ScYSZ anodes were exposed to H_2S in the ppm range both for short periods of 24h and for a few hundred hours. In a fuel containing significant shares of methane, the reforming activities of the Ni/YSZ and Ni/ScYSZ anodes were severely poisoned already at low H_2S concentrations of ~2ppm H_2S. The poisoning effect on the cell voltage was reversible only to a certain degree after exposure of 500 h in the state-of-the-art cell, due to a loss of percolation of Ni particles in the Ni/YSZ anode layers closest to the electrolyte. Using SOFCs with Ni/ScYSZ anodes improved the H_2S tolerance considerably, even at larger H_2S concentrations of 10 and 20ppm over a few hundred hours.
机译:氢以及含碳燃料的可用性是固体氧化物燃料电池(SOFC)的重要优势之一,这为使用衍生自常规资源(例如天然气)和可再生资源(例如沼气)的燃料提供了可能性。在这方面,诸如硫化合物之类的杂质至关重要。先进的Ni / YSZ SOFC阳极对硫杂质非常敏感。在当前的研究中,带有Ni / YSZ或Ni / ScYSZ阳极的阳极支撑的SOFC暴露在ppm范围内的H_2S中短时24小时和几百小时。在含有大量甲烷的燃料中,Ni / YSZ和Ni / ScYSZ阳极的重整活性已经在约2ppm H_2S的低H_2S浓度下严重中毒。在最先进的电池中暴露500小时后,对电池电压的中毒作用只能在一定程度上逆转,这是由于最接近电解质的Ni / YSZ阳极层中的Ni颗粒渗漏损失。将SOFC与Ni / ScYSZ阳极一起使用,即使在几百小时内甚至在10和20ppm的较大H_2S浓度下,也能显着提高H_2S耐受性。

著录项

  • 来源
    《Journal of power sources》 |2011年第17期|p.7271-7276|共6页
  • 作者单位

    Risoe DTU, Fuel Cells and Solid State Chemistry Division, Frederiksborgvej 399. DK 4000 Roskilde, Denmark;

    Risoe DTU, Fuel Cells and Solid State Chemistry Division, Frederiksborgvej 399. DK 4000 Roskilde, Denmark;

    Risoe DTU, Fuel Cells and Solid State Chemistry Division, Frederiksborgvej 399. DK 4000 Roskilde, Denmark;

  • 收录信息 美国《科学引文索引》(SCI);美国《工程索引》(EI);美国《生物学医学文摘》(MEDLINE);
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    sofc; h2s poisoning; methane; reforming; microscopy;

    机译:sofc;h2s中毒;甲烷改革显微镜检查;
  • 入库时间 2022-08-18 00:24:31

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号