A-type zeolite membranes were successfully synthesized on tubular alpha-Al2O3 supports by secondary growth method with vacuum seeding In the seeding process, a thin, uniform and continuous seeding layer was closely attached to the support surface by the pressure difference between the two sides of the support wall. The effects of seed particle size, suspension concentration, coating pressure difference and coating time on the membrane and its pervaporation properties were investigated. The as-synthesized membranes were characterized by XRD and SEM. The quality of the membranes was evaluated by the pervaporation dehydration of 95 wt. % isopropanol/water mixture at 343 K. High quality A-type zeolite membranes can be reproducibly prepared by the secondary growth method with vacuum seeding under the conditions: seed particle size of 500-1200 nm, suspension concentration of 4-8 g/l, coating pressure difference of 0.0100-0.0250 MPa and coating time of 45-180 s. (C) 2004 Elsevier B.V. All rights reserved.
机译:通过真空接种的二次生长方法,成功地在管状α-Al2O3载体上合成了A型沸石膜。在播种过程中,薄,均匀且连续的播种层通过两面之间的压差紧密附着在载体表面上。支撑墙。研究了种子粒径,悬浮液浓度,包衣压力差和包衣时间对膜及其渗透性能的影响。所合成的膜通过XRD和SEM表征。通过95wt。%的全蒸发脱水来评价膜的质量。 %异丙醇/水混合物的浓度为343K。可以通过二次生长法在以下条件下以真空接种法可再现地制备高质量的A型沸石膜:种子粒径为500-1200 nm,悬浮液浓度为4-8 g / l ,涂层压力差为0.0100-0.0250 MPa,涂层时间为45-180 s。 (C)2004 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号