In this study, porous alumina membranes were modified with two kinds of n-alkanoic acids (octanoic acid and octadecanoic acid) at different concentrations and reaction times for the preparation of hydrophobic membranes. The properties of the modified membranes were characterized by contact angle, attenuated total reflectance-Fourier transform infrared spectroscopy (ATR-FTIR) and electron spectroscopy for chemical analysis (ESCA), and the better modification condition was determined as reaction time of 20 min and concentration of 10 mM for both n-alkanoic acids. Furthermore, adsorption and desorption performances of bovine serum albumin (BSA) onto the modified membranes in the batch and flow processes were investigated. The saturation capacity was 0.003 μmol/cm~2 for the octanoic acid-modified membrane and 0.004 μmol/cm~2 for the octadecanoic acid-modified membrane, under the better modification condition. Liquid chromatography and fluorescence measurement were subsequently conducted to analyze the BSA properties during the adsorption and desorption stages. Finally, the flow performance of BSA was found to be limited by its slow adsorption and desorption rates.
机译:在这项研究中,用不同浓度和反应时间的两种正链烷酸(辛酸和十八烷酸)对多孔氧化铝膜进行改性,以制备疏水膜。通过接触角,全反射衰减-傅里叶红外光谱(ATR-FTIR)和化学分析电子光谱(ESCA)表征了改性膜的性能,确定了较好的改性条件为20min的反应时间和浓度。两种正链烷酸的最大分子量均为10 mM。此外,还研究了牛血清白蛋白(BSA)在分批和流动过程中对改性膜的吸附和解吸性能。在更好的改性条件下,辛酸改性膜的饱和容量为0.003μmol/ cm〜2,十八烷酸改性膜的饱和容量为0.004μmol/ cm〜2。随后进行液相色谱和荧光测量以分析吸附和解吸阶段的BSA特性。最后,发现BSA的流动性能受到其缓慢的吸附和解吸速率的限制。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号