Characterization of doxycycline-loaded calcium phosphate cement: implications for treatment of aneurysmal bone cysts

机译:强力霉素磷酸钙骨水泥的表征:对动脉瘤性骨囊肿的治疗意义

获取原文
获取原文并翻译 | 示例

摘要

Percutaneous doxycycline for treatment for aneurysmal bone cysts (ABCs) has been shown to decrease recurrence rates, however, this requires multiple procedures, includes the risks soft tissue necrosis, and does not provide structural support. We propose utilizing curettage with doxycycline-loaded calcium phosphate cement. This study aimed to evaluate the elution profile of doxycycline from calcium phosphate cement. Calcium phosphate cement underwent an in vitro elution protocol evaluating doxycycline concentrations of 0, 5, 10, and 15 mg/mL. Eluted concentrations were quantified utilizing high performance liquid chromatography at predetermined time points over 96 h. Compressive strength was evaluated both pre- and post-elution and micro-computed tomography was utilized to assess changes in cement porosity. Cement with 15 mg/mL of doxycycline maintained a higher average concentration (mean, 95% confidence intervals) (14.5 A mu g/mL [9.2-19.9 A mu g/mL]) compared to both 5 mg/mL (5.8 A mu g/mL [3.1-8.6 A mu g/mL]; P 0.001) and 10 mg/mL (8.4 +/- A mu g/mL [6.0-10.9 A mu g/mL]; P 0.001). Ultimate stress significantly decreased between pre- and post-elution samples for 10 mg/mL (P= 0.001) and 15 mg/mL (P = 0.004) groups. This study demonstrated a dose-dependent response in ultimate strength and compressive modulus with addition of doxycycline to calcium phosphate cement.
机译:经皮多西环素治疗动脉瘤性骨囊肿(ABC)已显示可降低复发率,但是,这需要多次手术,包括软组织坏死的风险,并且不提供结构支持。我们建议使用多西环素负载的磷酸钙水泥进行刮宫术。本研究旨在评估强力霉素从磷酸钙水泥中的洗脱曲线。磷酸钙水泥经过体外洗脱,评估多西环素的浓度为0、5、10和15 mg / mL。使用高效液相色谱仪在96小时内的预定时间点对洗脱浓度进行定量。在洗脱之前和之后都评估了抗压强度,并使用了计算机断层扫描技术来评估水泥孔隙率的变化。与5 mg / mL(5.8 A mu)相比,含15 mg / mL强力霉素的水泥保持较高的平均浓度(平均值,95%置信区间)(14.5 Aμg / mL [9.2-19.9 A mu g / mL])。 g / mL [3.1-8.6 Aμg / mL]; P <0.001)和10 mg / mL(8.4 +/- Aμg / mL [6.0-10.9 Aμg / mL]; P <0.001)。在10 mg / mL(P = 0.001)和15 mg / mL(P = 0.004)组的洗脱前和洗脱后样品之间,最终应力显着降低。这项研究表明,在磷酸钙水泥中添加强力霉素可达到最终强度和压缩模量的剂量依赖性响应。

著录项

  • 来源
    《Journal of materials science 》 |2018年第7期| 109.1-109.6| 共6页
  • 作者单位

    Beaumont Hlth, Dept Orthopaed Surg, 3601 W 13 Mile Rd, Royal Oak, MI 48073 USA;

    Beaumont Hlth, Dept Orthopaed Surg, 3601 W 13 Mile Rd, Royal Oak, MI 48073 USA;

    Beaumont Hlth, Dept Orthopaed Surg, 3601 W 13 Mile Rd, Royal Oak, MI 48073 USA;

    Beaumont Hlth, Dept Orthopaed Surg, 3601 W 13 Mile Rd, Royal Oak, MI 48073 USA;

  • 收录信息
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号