Abstract In the present work, the glass systems 0.70TeO2–0.30MO and 0.65TeO2–0.35MO (M = Ba, Sr) were prepared and characterized by X-ray diffraction, Fourier transform infrared spectroscopy, UV–vis spectroscopy and differential scanning calorimetry. The structural studies show that amorphous alkaline tellurite glasses are made up of vibrational units of molecular water group, hydroxyl bonding, symmetrical stretching vibration of Te–Oax bonds in the deformed TeO4 and stretching and bending vibration of Te–O–Te linkages in TeO4/TeO3 + d polyhedra/TeO3. In the X-ray diffractograms, shifting of amorphous peak was observed towards higher angle side with the strontium substitution in comparison to barium substitution due to lower ionic radii. The optical band gap of investigated glasses was found to lie in the range 2.94–3.31 eV and was found to be lower in SrO added glasses than that of BaO added glasses. This may be due to the presence of more number of non-bridging oxygen in Sr substituted glasses than Ba substituted glasses. The Ba substituted samples were observed to be denser than Sr substituted glasses. Ultrasonic longitudinal and sheer velocities were found in the range of 3160–3210 and 1785–1850 m/s, respectively and were observed to be higher in Ba substituted glasses. The ac conductivity spectra were found to follow Jonscher power law and conduction mechanism is governed by overlapping large polaron tunneling model created with non-bridging oxygen and Tellurium ions.
机译:摘要 在当前工作中,玻璃系统0.70TeO 2 –0.30MO和0.65TeO 2 –0.35MO(M = Ba (Sr)制备,并通过X射线衍射,傅里叶变换红外光谱,UV-vis光谱和差示扫描量热法进行表征。结构研究表明,非晶态碱金属碲酸盐玻璃是由分子水基的振动单元,羟基键,变形的TeO 4 ax 键的对称拉伸振动组成。 >和TeO 4 / TeO 3 + d 多面体/ TeO 3 中Te–O–Te键的伸缩振动。在X射线衍射图中,与钡取代相比,由于较低的离子半径,观察到无定形峰在锶取代下向较高角度侧移动。发现所研究的玻璃的光学带隙在2.94–3.31eV范围内,并且发现添加SrO的玻璃的带隙比添加BaO的玻璃的带隙低。这可能是由于在Sr取代的玻璃中比在Ba取代的玻璃中存在更多的非桥接氧。观察到Ba取代的样品比Sr取代的玻璃致密。超声波的纵向和剪切速度分别在3160–3210和1785–1850 m / s的范围内,并且在Ba替代玻璃中观察到的更高。交流电导率谱符合Jonscher幂定律,其传导机制受非桥接氧和碲离子重叠的大极化子隧穿模型控制。

著录项

  • 来源
    《Journal of materials science 》 |2017年第10期| 7419-7428| 共10页
  • 作者单位

    Department of Physics, Dr. Bheem Rao Ambedkar Government Degree College;

    Department of Physics, Indian Institute of Technology (Banaras Hindu University);

    Department of Physics, Indian Institute of Technology (Banaras Hindu University);

  • 收录信息 美国《科学引文索引》(SCI);美国《工程索引》(EI);美国《生物学医学文摘》(MEDLINE);
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号