首页> 外文期刊>Journal of materials in civil engineering >Low-Volume Road WMA Mixtures: Moisture Susceptibility of Mixtures Containing Coal Ash and Roofing Shingle with Moist Aggregate
【24h】

Low-Volume Road WMA Mixtures: Moisture Susceptibility of Mixtures Containing Coal Ash and Roofing Shingle with Moist Aggregate

机译:小体积道路WMA混合物:含煤灰和屋面瓦与湿骨料的混合物的水分敏感性

获取原文
获取原文并翻译 | 示例
           

摘要

The objective of this study was to evaluate the laboratory moisture susceptibility of low-volume hot mix asphalt (HMA) and warm mix asphalt (WMA) mixtures containing moist aggregates and recycled materials, such as manufactured roofing shingles and coal ash material. These materials were tested after short- and long-term aging procedures. The test properties of these mixtures included indirect tensile strength (ITS), the tensile strength ratio (TSR), and the flow value of virgin and aged specimens. The experimental design included two percentages of coal ash (10 and 5% by weight of the aggregate), two roofing shingle contents (5 and 3% by weight of the aggregate), three WMA additives (Asphamin, Sasobit, and Evotherm), two antistripping agents (hydrated lime and one liquid antistripping agent), and two aggregate sources. A total of 72 mixtures were designed and a total of 416 ITS specimens were tested for short- and long-term aged procedures in this study. The test results indicated that the dry and wet ITS values of low-volume mixtures containing moist aggregate generally satisfied the demand of pavement without requiring additional treatment. Mixtures containing hydrated lime, in general, showed a better moisture resistance than liquid ASA for WMA mixtures. Moreover, the addition of WMA additives in the low-volume mixture was effective and generally showed a similar moisture resistance to HMA, except for when using Asphamin and liquid ASA simultaneously. Research results also indicated that the utilization of recycled coal ash and roofing shingles significantly improved moisture resistance of HMA and WMA mixtures
机译:这项研究的目的是评估实验室的低湿热混合沥青(HMA)和温混合沥青(WMA)混合物的湿气敏感性,这些混合物包含潮湿的骨料和回收材料,例如人造屋顶板和煤灰材料。这些材料在短期和长期老化程序之后进行了测试。这些混合物的测试特性包括间接拉伸强度(ITS),拉伸强度比(TSR)以及原始样品和老化样品的流量值。实验设计包括2%的煤灰(占骨料的10%和5%),两种屋面瓦含量(占骨料的5%和3%),三种WMA添加剂(沥青,Sasobit和Evotherm),两种抗剥落剂(熟石灰和一种液体抗剥落剂)和两种集料来源。本研究共设计了72种混合物,并测试了416种ITS标本的短期和长期老化程序。测试结果表明,含湿骨料的小体积混合物的干,湿ITS值通常可以满足路面需求,而无需其他处理。通常,对于WMA混合物,含熟石灰的混合物显示出比液态ASA更好的耐湿性。此外,在少量混合物中添加WMA添加剂是有效的,并且通常显示出与HMA相似的耐湿性,除了同时使用Asphamin和液态ASA时。研究结果还表明,利用回收的煤灰和屋顶瓦可以显着提高HMA和WMA混合物的耐湿性

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号