The effect of mixture composition and coarse aggregate density on the shear strength and cracking behavior of self-consolidating concrete (SCC) beams are presented in this study. The experimental test parameters included coarse/fine (C/F) aggregate ratio (ranging from 0.7 to 1.2), coarse aggregate size (10 and 20 mm), coarse aggregate type/density (slag, expanded slate, and crushed stone), and varying compressive strengths (26-72 MPa). The density of the tested mixtures varied from 1,848 to 2,286 kg/m~3. The study investigates the fresh properties of all tested mixtures and the shear strength and cracking behavior of 16 full-scale concrete beams. Based on some selected design codes, the ultimate shear strength of the tested beams is also predicted. The results showed that SCC mixtures with a higher C/F ratio or bigger normal-weight aggregate had better flowability and less high range water reducer admixtures (HRWRA) demand. Although all tested beams showed comparable normalized shear strength, beams with a high C/F ratio or bigger normal-weight aggregate had higher post-diagonal cracking resistance. The results also showed that the expanded slate and slag lightweight aggregates were found to be relatively strong (compared to most common lightweight aggregates) as they did not entirely break along the diagonal crack. Increasing the volume of these lightweight aggregates in SCC mixtures not only reduced the mixture density but also enhanced the postdiagonal cracking resistance.
机译:提出了混合料组成和粗骨料密度对自密实混凝土(SCC)梁的抗剪强度和抗裂性能的影响。实验测试参数包括粗/细(C / F)骨料比率(范围为0.7至1.2),粗骨料尺寸(10和20毫米),粗骨料类型/密度(矿渣,膨胀板岩和碎石),以及各种抗压强度(26-72 MPa)。被测混合物的密度为1,848至2,286 kg / m〜3。该研究调查了所有测试混合物的新鲜特性以及16条全尺寸混凝土梁的抗剪强度和抗裂性能。根据一些选定的设计规范,还可以预测被测梁的极限抗剪强度。结果表明,具有较高C / F比或更大的标准重量骨料的SCC混合物具有较好的流动性和较少的高范围减水剂(HRWRA)需求。尽管所有测试梁均显示出可比的归一化剪切强度,但具有高C / F比或更大的标准重量骨料的梁具有更高的对角后抗裂性。结果还显示,发现膨胀的板岩和矿渣轻质骨料相对较强(与大多数常见的轻质骨料相比),因为它们没有完全沿着对角线裂缝破裂。增加这些轻质骨料在SCC混合物中的体积,不仅降低了混合物的密度,而且增强了对角线后抗裂性。

著录项

  • 来源
    《Journal of materials in civil engineering》 |2015年第11期|04015022.1-04015022.11|共11页
  • 作者单位

    Faculty of Engineering and Applied Science, Memorial Univ. of Newfoundland, St. John's, Newfoundland, Canada A1B 3X5;

    Faculty of Engineering and Applied Science, Memorial Univ. of Newfoundland, St. John's, Newfoundland, Canada A1B 3X5;

    Faculty of Engineering and Applied Science, Memorial Univ. of Newfoundland, St. John's, Newfoundland, Canada A1B 3X5;

  • 收录信息
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号