Liquid antistripping agents are added to asphalt binder to improve moisture resistance of the mixture. However, the chemical makeup and bonding mechanism of antistripping agents may cause significant effects on binder rheology. This paper investigates the effects of two different liquid antistripping agents, one amine based and another silane based, on the rheological properties of crumb rubber-modified binder CRMB60. Rheological properties determined included rotational viscosity, performance grade (PG), percent recovery, nonrecoverable creep compliance, creep stiffness, and rate of relaxation. The number of cycles to fatigue failure aided in evaluating the fatigue life. The results show that the addition of antistripping agents caused a decrease in rotational viscosity of CRMB60. Moreover, the silane antistripping agent was observed to cause a bump in high-temperature PG, whereas low-temperature PG remained unaffected by both antistripping agents. The multiple stress creep and recovery (MSCR) analysis exhibited that the silane antistripping agent increased the percent recovery and decreased the nonrecoverable creep compliance, whereas the contrary trend was observed with addition of the amine antistripping agent. Both the amine and silane antistripping agents caused a significant decrease in the fatigue life of CRMB60. Additionally, minor effect was observed on low-temperature cracking performance by both the amine and silane antistripping agents up to a certain temperature below which the cracking exacerbates. Overall, it was concluded that antistripping agents affect the rheology of CRMB60 and should be given due consideration prior to adopting a particular antistripping agent.
机译:将液体防剥离剂添加到沥青粘合剂中,以改善混合物的耐湿性。但是,防剥离剂的化学组成和键合机理可能会对粘合剂的流变性产生重大影响。本文研究了两种不同的液体防剥离剂,一种胺基和另一种硅烷基,对生胶改性粘合剂CRMB60的流变性能的影响。确定的流变性质包括旋转粘度,性能等级(PG),恢复百分数,不可恢复的蠕变柔度,蠕变刚度和松弛率。疲劳破坏的循环次数有助于评估疲劳寿命。结果表明,抗剥离剂的加入导致CRMB60的旋转粘度降低。此外,观察到硅烷抗剥离剂在高温PG中引起碰撞,而低温PG保持不受两种抗剥离剂的影响。多重应力蠕变和恢复(MSCR)分析表明,硅烷抗剥离剂提高了恢复百分率,降低了不可恢复的蠕变顺应性,而添加胺抗剥离剂则观察到相反的趋势。胺类和硅烷类防剥离剂均导致CRMB60的疲劳寿命显着降低。另外,在一定温度下,胺和硅烷抗汽提剂对低温裂化性能的影响很小,在该温度以下,裂化加剧。总的来说,得出的结论是,抗剥离剂会影响CRMB60的流变性,在采用特定的抗剥离剂之前应给予应有的考虑。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号