Stearyl alcohol/2,4-toluene diisocyanate/perfluorinated alcohols adduct was prepared at a total conversion of 98% by reacting these substances using a molar ratio of 1/1/1 at 100℃ for 90 minutes. The purified adduct has a melting point of 67℃, and its FTIR spectrum was investigated. An aqueous emulsion containing the adduct (105 g/kg), stearic acid (45 g/kg), and TEA (24 g/kg) acquired 100% cotton fabric water/oil repellency when padded in a bath containing different concentration (20-50 g/L) of the emulsion and dried at 100℃ per 3 minutes. Raising drying temperature (100-180℃) enhanced water/oil repellency. The so-treated fabric lost water/oil repellency after five washes. Addition of DMDHEU to the padding bath relatively improved water/oil repellency up to the 10th wash, but it was completely lost after the 25th wash. It was concluded that the adduct is mechanically entrapped within the crosslinker/fabric network and it escapes this entrapment during repeated laundering.
机译:硬脂醇/ 2,4-甲苯二异氰酸酯/全氟醇加合物的制备是通过使这些物质在100℃下以1/1/1的摩尔比反应90分钟而使总转化率达到98%。纯化的加合物的熔点为67℃,并对其FTIR光谱进行了研究。含有加合物(105 g / kg),硬脂酸(45 g / kg)和TEA(24 g / kg)的水乳液在填充到不同浓度的浴中时具有100%的棉织物拒水拒油性(20- 50 g / L)的乳液,并在100℃下每3分钟干燥一次。提高干燥温度(100-180℃)可提高拒水拒油性。经过五次洗涤后,如此处理的织物失去了拒水拒油性。在填充浴中添加DMDHEU可以提高至第10次洗涤的拒水拒油性,但在第25次洗涤后完全消失。结论是,加合物被机械截留在交联剂/织物网络中,并且在反复洗涤期间其逃脱了这种夹带。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号