The migration of metals (e.g., Fe, Cd, Co, Cr, Cu, Mn, Ni, and Zn) in both of iron tailings under different pH leachates was studied by laboratory static leaching experiments. The results indicated that Fe showed the highest leaching concentration at an initial pH of 2, reaching 16.19 and 51.72 mg L-1 in the Qian'anling (Q0) and Majuanzi (M0) iron tailings, respectively. Metal ions manifested a strong pH dependence. In addition, the leaching behavior of Cd, Cr, Fe, and Cu for the two tailings was also evaluated under leaching by three low-molecular-weight organic acids (LMWOAs). The results indicated the leaching of Cd and Fe followed the order of citric acid > malic acid > oxalic acid and that the leaching order for Cr and Cu was citric acid > oxalic acid > malic acid. The concentration of Fe was low in 5 mM oxalic acid leaching for 20 days because of the hydrolysis precipitation of iron ions and the complexation with organic ligand. The crystal lattice on the tailings was significantly damaged after leaching. The CO32- peak appeared in MO with different treatments, and the proportion of COO- fitting peak areas increased markedly after leaching with LMWOAs.
机译:通过实验室静态浸出实验研究了不同pH浸出液中铁尾矿中金属(例如Fe,Cd,Co,Cr,Cr,Cu,Mn,Ni和Zn)的迁移。结果表明,在迁安岭(Q0)和马娟子(M0)铁尾矿中,Fe在初始pH为2时显示出最高的浸出浓度,分别达到16.19和51.72 mg L-1。金属离子表现出强烈的pH依赖性。此外,还通过三种低分子量有机酸(LMWOA)的浸出评价了Cd,Cr,Fe和Cu对两种尾矿的浸出行为。结果表明,Cd和Fe的浸出顺序为柠檬酸>苹果酸>草酸,Cr和Cu的浸出顺序为柠檬酸>草酸>苹果酸。由于铁离子的水解沉淀和与有机配体的络合,在5 mM草酸浸出20天中,Fe的浓度较低。浸出后,尾矿上的晶格明显受损。用LMWOAs浸出后,MO处理中的CO32-峰出现在MO中,COO适合峰面积的比例显着增加。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号