Leaching and geochemical behavior of fired bricks containing coal wastes

机译:含煤渣的烧结砖的浸出和地球化学行为

获取原文
获取原文并翻译 | 示例
       

摘要

High amounts of mine wastes are continuously produced by the mining industry all over the world. Recycling possibility of some wastes in fired brick making has been investigated and showed promising results. However, little attention is given to the leaching behavior of mine wastes based fired bricks. The objective of this paper is to evaluate the geochemical behavior of fired bricks containing different types of coal wastes. The leachates were analyzed for their concentration of As, Ba, Cd, Co, Cr, Cu, Mo, Ni, Pb, Zn and sulfates using different leaching tests; namely Tank Leaching tests (NEN 7375), Toxicity Characteristic Leaching Procedure (TCLP) and pH dependence test (EPA, 1313). The results showed that the release of constituents of potential interest was highly reduced after thermal treatment and were immobilized within the glassy matrix of the fired bricks. Moreover, it was also highlighted that the final pH of all fired samples changed and stabilized around 8–8.5 when the initial pH of leaching solution was in the range 2.5–11.5. The release of heavy metals and metalloids (As) tended to decrease with the increase of pH from acidic to alkaline solutions while Mo displayed a different trend.
机译:世界各地的采矿业不断产生大量的矿山废物。已经研究了烧制砖中一些废物的再循环可能性,并显示出令人鼓舞的结果。然而,很少有人关注基于矿渣的烧砖的浸出行为。本文的目的是评估含有不同类型煤炭废物的烧结砖的地球化学行为。使用不同的浸出试验分析渗滤液的砷,钡,镉,钴,铬,铜,钼,镍,铅,锌和硫酸盐的浓度。分别是储罐浸出测试(NEN 7375),毒性特征浸出程序(TCLP)和pH依赖性测试(EPA,1313)。结果表明,潜在感兴趣的成分的释放在热处理后被大大降低,并被固定在烧结砖的玻璃状基质中。此外,还需要强调的是,当浸出溶液的初始pH值在2.5-11.5范围内时,所有焙烧样品的最终pH值均发生变化并稳定在8-8.5附近。随着pH从酸性溶液向碱性溶液的增加,重金属和准金属(As)的释放趋于减少,而Mo呈现出不同的趋势。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号