Structural connections in bridges supporting directly the railway track have cumulated large amount of load cycles from passing trains. The connections were not originally designed for fatigue and some of them have found to be in poor condition by inspection. To study their structural behaviour under large number of repeated load cycles, five 85 year old stringer-to-floorbeam connections from a decommissioned railway bridge were loaded in laboratory. Each connection had four angle plates connecting stringer webs to floorbeams and two connection plates connecting stringer top flanges together. During the load tests, the connection plate maximum stress ranged from 60 MPa to 150 MPa. It was estimated that the peak stresses under traffic were in the range of 40-60 MPa. Despite large stresses in load tests and long active use under traffic, only three connections failed after 0.5-1.6 million load cycles. Two connection tests were run out after 2.4 and 2.6 million cycles. By measuring strains and displacements continuously during testing it was seen that failures occurred gradually as components fractured slowly during tens of thousands of cycles. Any of the connection failures was not complete and the connections showed substantial residual bending stiffness and capacity after failure. Load tests showed that even if connection is seen to be in poor condition and close to its theoretical fatigue life, it still might function safely for hundreds of thousands of stress cycles if stress redistribution between connection components is possible and connection is monitored for major fractures. (C) 2019 Elsevier Ltd. All rights reserved.
机译:直接支撑铁路轨道的桥梁中的结构连接累计了来自过往列车的大量载荷循环。连接最初不是为疲劳而设计的,经检查发现其中一些状态不佳。为了研究它们在大量重复荷载循环下的结构性能,在实验室中对来自退役铁路桥梁的五个85年的桁梁至楼板连接进行了荷载。每个连接具有四个将纵梁腹板连接到地板梁的角板,以及两个将纵梁顶部凸缘连接在一起的连接板。在负载测试期间,连接板的最大应力范围为60 MPa至150 MPa。据估计,交通中的峰值应力在40-60 MPa的范围内。尽管在负载测试中承受了很大的压力,并且在流量下长期活跃使用,但是在0.5-160万个负载周期后,只有三个连接失败。在2.4和260万次循环后进行了两次连接测试。通过在测试过程中连续测量应变和位移,可以看到随着零件在数万次循环中缓慢破裂,故障逐渐发生。任何连接故障均未完成,并且连接在故障后显示出相当大的残余弯曲刚度和承载能力。负载测试表明,即使连接处处于不良状态并接近其理论疲劳寿命,但如果可能在连接组件之间重新分配应力并监视连接处的重大断裂,即使在数十万次应力循环中,连接仍可以安全运行。 (C)2019 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号