Refused derived fuel from municipal solid waste used as an alternative fuel during the iron ore sinter process

机译:拒绝从城市固体废物中使用的燃料,用作铁矿石烧结过程中的替代燃料

获取原文
获取原文并翻译 | 示例
       

摘要

In order to reduce the fuel cost of the steel company and dispose municipal solid waste (MSW), refused derived fuel (RDF) was prepared by MSW carbonization and used as an alternative fuel in the sinter process of the steel company. The calorific value of MSW carbonized under 500 degrees C (designed as RDF-500) was 25.47 MJ kg(-1), and its ash content and volatile matter was 15.1% and 21.3%, respectively. The properties of RDF-500 were more close to those of coke breeze. Hence, RDF-500 was regarded as the alternative fuel in the iron ore sinter process. The experimental results demonstrated that the qualities (yield, tumble strength index and shatter strength index) of the sintered ore were not significantly decreased until the replacement ratio of RDF-500 was above 20%. The tumble strength index and shatter strength index of the sintered ore under 20% RDF-500 replacement ratio were 62.58% and 60.93%, which were little lower than those with full coke breeze (65.78% and 63.43%). RDF-500 contained more volatile matter, which was unuseful for forming the liquid phase of the mineral matter. Thus, the duration of temperature for mineral melting (DTMM) and liquid phase formation area (LPFA) were decreased when RDF-500 was used to replace part of coke breeze, which accounted for the decrease of the qualities of the sintered ore. In addition, more CO and NOx were emitted and less SO2 was formed when 20% coke breeze was replaced with RDF-500. (C) 2020 Elsevier Ltd. All rights reserved.
机译:为了降低钢铁公司的燃料成本并使城市固体废物(MSW),通过MSW碳化制备拒绝衍生的燃料(RDF),并用作钢铁公司烧结过程中的替代燃料。 500摄氏度(设计为RDF-500)的MSF的热量值为25.47mJ kg(-1),其灰分含量和挥发物质分别为15.1%和21.3%。 RDF-500的性质更接近焦炭微风。因此,RDF-500被认为是铁矿石烧结过程中的替代燃料。实验结果表明,烧结矿石的质量(产量,滚石强度指数和破碎强度指数)在RDF-500的替代比率高于20%之前,不会显着降低。烧结矿石的倾斜强度指数和粉碎的矿石下降20%RDF-500置换率率为62.58%和60.93%,与全焦微风(65.78%和63.43%)小。 RDF-500含有更多的挥发性物质,这对形成矿物质的液相是不使用的。因此,当RDF-500用于代替部分焦炭微风时,降低了矿物熔化(DTMM)和液相形成区域(LPFA)的温度持续时间,这考虑了烧结矿石的品质的降低。此外,当用RDF-500代替20%的焦炭微血时,形成更多CO和NOx,并且当用RDF-500代替20%的焦炭微血时,形成较少的SO 2。 (c)2020 elestvier有限公司保留所有权利。

著录项

  • 来源
    《Journal of Cleaner Production》 |2021年第1期|123594.1-123594.8|共8页
  • 作者单位

    Wuhan Univ Sci & Technol Hubei Key Lab Efficient Utilizat & Agglomerat Met Wuhan 430081 Peoples R China;

    Wuhan Univ Sci & Technol Hubei Key Lab Efficient Utilizat & Agglomerat Met Wuhan 430081 Peoples R China;

    Wuhan Univ Sci & Technol Hubei Key Lab Efficient Utilizat & Agglomerat Met Wuhan 430081 Peoples R China;

    Wuhan Univ Sci & Technol Hubei Prov Ind Safety Engn Technol Res Ctr Wuhan 430081 Peoples R China;

    Wuhan Univ Sci & Technol Hubei Key Lab Efficient Utilizat & Agglomerat Met Wuhan 430081 Peoples R China;

    Wuhan Univ Sci & Technol Hubei Key Lab Efficient Utilizat & Agglomerat Met Wuhan 430081 Peoples R China;

  • 收录信息
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    MSW; Pyrolysis; RDF; Coke breeze; Replacement; Sinter;

    机译:MSW;热解;RDF;可乐微风;更换;烧结;