Alkali-activated cements (AACs) technology is being widely investigated as a replacement for ordinary Portland cement (OPC) for environmental benefits. Blast furnace slag (BFS) is one of the most well known precursors used in AACs, having comparable properties to those of traditional OPC-based materials. AACs require alkali solutions, which are commonly based on a combination of sodium or potassium hydroxides with sodium or potassium silicates in high concentration. These alkali solutions represent the use of chemical reagents, and thus can have major environmental, health and economic impacts. Olive-stone (also known as olive pits) biomass ash (OBA) is a residue mainly composed of calcium and potassium oxides. Rice husk ash (RHA) is a rich silica residue from the combustion of rice husk. The combination of both residues can produce a good activating reagent for BFS-based AACs. In the present work, 100% waste-based ternary alkali-activated mortars (TAAM) based on BFS activated by OBA and RHA were developed. The mortars were assessed in terms of their dosage, curing treatment and time evolution. Finally an eco-friendly 100% waste-based TAAM with 67.39 +/- 0.44 MPa after 90 days of curing at 20 degrees C is obtained and a complete microstructural characterization shows a dense and compact matrix with binding gel products labelled as C(K)-S(A)-H and C(K)-S-H. (C) 2019 Elsevier Ltd. All rights reserved.
机译:碱活化水泥(AACs)技术正在被广泛研究,以替代普通波特兰水泥(OPC),以提高环境效益。高炉矿渣(BFS)是AAC中使用的最著名的前体之一,其性能与传统的基于OPC的材料相当。 AAC需要碱溶液,通常基于氢氧化钠或氢氧化钾与高浓度硅酸钠或硅酸钾的组合。这些碱性溶液代表了化学试剂的使用,因此可能会对环境,健康和经济产生重大影响。橄榄石(也称为橄榄核)生物质灰分(OBA)是主要由钙和钾氧化物组成的残渣。稻壳灰(RHA)是稻壳燃烧产生的富含二氧化硅的残留物。这两个残基的结合可以为基于BFS的AAC产生良好的活化剂。在目前的工作中,开发了基于OBA和RHA活化的BFS的100%废物基三元活化灰浆(TAAM)。根据砂浆的用量,固化处理和时间演变对其进行评估。最终,在20摄氏度下固化90天后,获得67.39 +/- 0.44 MPa的100%废物型环保TAAM,完整的微观结构表征显示出致密而致密的基质,结合凝胶产物标记为C(K) -S(A)-H和C(K)-SH。 (C)2019 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号