Recycling of steel plant mill scale via iron ore pelletisation process

机译:通过铁矿石造粒工艺回收钢铁厂的氧化皮

获取原文
获取原文并翻译 | 示例

摘要

Mill scale is an iron oxide waste generated during steelmaking, casting and rolling. Total generation of mill scale at JSWSL is around 150 t/day and contains 60-70%FeO and 30-35%Fe2O3. To recover the iron, the mill scale must be smelted in a blast furnace or other reduction furnace; however, it is usually too fine to use without previous agglomeration such as via pellet or sinter mix. JSWSL operates a 4·2 Mtpa pellet plant to produce pellets for Corex and BF ironmaking units. The aim of this study is to determine the effect of mill scale on pellet properties. Detailed laboratory basket trials were conducted using up to 40% of mill scale in the pellet mix. The addition of mill scale up to 10% is considered to provide the optimum balance of chemical, physical and metallurgical properties of the pellet.
机译:氧化皮是炼钢,铸造和轧制过程中产生的氧化铁废物。 JSWSL的总规模为150吨/天,其中包含60-70%FeO和30-35%Fe 2 O 3 。为了回收铁,必须在高炉或其他还原炉中冶炼氧化皮。但是,如果事先没有附聚(例如通过粒料或烧结混合料)而使用,通常太好了。 JSWSL运营一家4·2 Mtpa球团厂,为Corex和高炉炼铁装置生产球团。这项研究的目的是确定工厂规模对颗粒性质的影响。进行了详细的实验室篮试验,使用的是颗粒混合物中高达40%的工厂规模。可以考虑添加高达10%的轧机氧化皮,以使颗粒的化学,物理和冶金性能达到最佳平衡。

著录项

  • 来源
    《Ironmaking & Steelmaking》 |2009年第6期|409-415|共7页
  • 作者单位

    JSW Steel Ltd, Torangallu, Vidyanagar, Bellary, Karnataka, India;

    JSW Steel Ltd, Torangallu, Vidyanagar, Bellary, Karnataka, India;

    JSW Steel Ltd, Torangallu, Vidyanagar, Bellary, Karnataka, India;

    JSW Steel Ltd, Torangallu, Vidyanagar, Bellary, Karnataka, India;

    JSW Steel Ltd, Torangallu, Vidyanagar, Bellary, Karnataka, India;

  • 收录信息
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号