Deformation behaviour of A356, Al-11Si-2.5Cu-0.6Fe, and Al-18Si-2.5Cu-0.6Fe alloys forged under different processing conditions

机译:在不同加工条件下锻造的A356,Al-11Si-2.5Cu-0.6Fe和Al-18Si-2.5Cu-0.6Fe合金的变形行为

获取原文
获取原文并翻译 | 示例
           

摘要

The present paper aims to investigate the feasibility of bulk processing of Al-Si alloys under different processing temperatures. Three different compositions of Al-Si alloys (namely A356, Al-11Si-2.5Cu-0.6Fe, and Al-18Si-2.5Cu-0.6Fe) have been forged between flat die platen at 300 and 500°C processing temperatures. High-speed forging was performed with the help of power hammer. The results obtained are discussed critically to illustrate the interaction of various processing parameters associated with the processing of the alloys. The results reveal severe crack generation on the outer periphery of forged billets, while it reduced with low amount of silicon in the alloy. During processing, microstructural refinement and improvement in the mechanical properties were observed. The present work provides valuable insight into producing complex formed products of Al-Si alloys for extensive industrial applications.
机译:本文旨在研究在不同处理温度下进行Al-Si合金整体加工的可行性。在300和500°C的加工温度下,已在平板模板之间锻造了三种不同成分的Al-Si合金(即A356,Al-11Si-2.5Cu-0.6Fe和Al-18Si-2.5Cu-0.6Fe)。借助动力锤进行高速锻造。严格讨论了获得的结果,以说明与合金加工相关的各种加工参数之间的相互作用。结果表明,在锻造坯料的外围会产生严重的裂纹,而在合金中硅含量较低时,裂纹会减少。在加工过程中,观察到微结构的细化和机械性能的改善。目前的工作为生产用于广泛工业应用的复杂的铝硅合金成形产品提供了宝贵的见识。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号