Freeze-thaw cycling under a calcium chloride environment: effects on CFRP strengthened concrete structures

机译:氯化钙环境下的冻融循环:对CFRP加固混凝土结构的影响

获取原文
获取原文并翻译 | 示例
       

摘要

The fracture mechanics specimen known as the Single Contoured-Cantilever Beam (SCCB) - an experimental approach designed to ascertain both qualitative and quantitative information about the integrity of Fibre Reinforced Polymer (FRP) laminate-to-concrete interface bonds - has been used to assess the detrimental effects of subjecting concrete structures externally strengthened with Carbon Fibre Reinforced Polymer (CFRP) sheets to a combined thermo-chemical environment involving Freeze-Thaw (FT) cycling under a calcium chloride (CaCl_2) solution. Quantitative fracture measurements in terms of the Mode I critical strain energy release rates (G_(Ic)) were recorded after 50, 100, 150, 200 and 300 cycles of alternate freezing and thawing; moreover, specimen weights and strains were measured initially and at the end of every 5th cycle. Considerable degradation of the interface bond integrity was found to have resulted, particularly for the latter-stage cycled beams.
机译:称为单轮廓悬臂梁(SCCB)的断裂力学样本-一种用于确定关于纤维增强聚合物(FRP)层合混凝土界面粘结完整性的定性和定量信息的实验方法,已用于评估碳纤维增强聚合物(CFRP)板在外部加固的混凝土结构受到热化学环境的不利影响,其中包括在氯化钙(CaCl_2)溶液中进行的冻融(FT)循环。在交替冷冻和解冻50、100、150、200和300次循环后,记录了根据模式I临界应变能释放速率(G_(Ic))进行的定量断裂测量。此外,最初和每第5个循环结束时都要测量样品的重量和应变。发现导致界面键完整性的相当大的降低,特别是对于后期循环梁。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号