Quasi-static compressive testing of extruded aluminum alloy AA6061-T6 round and square cross-sectional tubular specimens was completed to investigate the crush characteristics of these structural members under a cutting deformation mode by using a specially designed cutting tool. Results from the experimental tests showed that the cutting deformation mode of the round and square tubes exhibited high crush force efficiencies (CFE) of 0.95 and 0.81 respectively. In comparison, CFE of round specimens that experienced progressive folding and global bending deformation modes were observed to be 0.66 and 0.20 respectively and CFE of square specimens that underwent global bending were found to be 0.22. An almost constant cutting force was observed for the round tubes in the cutting deformation mode, while a slight increase in the cutting force was observed for the square tubes under the same deformation mode. The increase in cutting force for the square tubes was observed to occur primarily due to contact arising between the cutting tool and tube sidewalls and to a lesser extent due to bending of the petalled side walls. For the round tubes, contact between the cutting tool and sidewalls as well as bending of the petalled side walls was not as significant and resulted in a more consistent cutting force. For both the 200 mm and 300 mm length tubes the total energy absorption for the round and square tubes was observed to be 6.11 kJ and 4.31 kJ respectively. The energy absorption was observed to be independent of tube length.
机译:完成了挤压铝合金AA6061-T6圆形和方形截面管状试样的准静态压缩试验,以研究使用特殊设计的切削工具在切削变形模式下这些结构构件的破碎特性。实验结果表明,圆管和方管的切削变形模式分别显示出0.95和0.81的高破碎力效率(CFE)。相比之下,圆形试样的渐进折叠和整体弯曲变形模式的CFE分别为0.66和0.20,经历整体弯曲的方形试样的CFE为0.22。在切削变形模式下,圆管的切削力几乎恒定,而在相同变形模式下,方管的切削力略有增加。观察到方形管切割力的增加主要是由于切割工具与管侧壁之间的接触而引起的,而较小的程度是由于瓣状侧壁的弯曲而引起的。对于圆管,切削工具与侧壁之间的接触以及瓣状侧壁的弯曲没有那么明显,并且导致了更一致的切削力。对于长度为200 mm和300 mm的管,圆形和方形管的总能量吸收分别为6.11 kJ和4.31 kJ。观察到能量吸收与管长无关。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号